Comparing lithography methods at DTU Danchip
| UV Lithography | DUV Stepper Lithography | E-beam Lithography | Nano Imprint Lithography | 2-Photon Polymerization Lithography | |
|---|---|---|---|---|---|
| Generel description | Generel description - method 1 | Generel description - method 2 | Electron beam lithography | 4 | 5 |
| Pattern size range |
|
|
|
|
|
| Resist type |
|
|
|
|
|
| Resist thickness range |
|
|
|
|
|
| Typical exposure time |
2s-30s pr. wafer |
?-? pr. ? |
Depends on dose, Q [µC/cm2], beam current, I [A], and pattern area, A [cm2]: t = Q*A/I |
? pr. wafer |
? pr. µm2 |
| Substrate size |
|
|
We have cassettes that fit to
Only one cassette can be loaded at time |
|
|
| Allowed materials |
|
|
|
|
|