On the L-drive, a logbook for the e-beam writer can be found. Sheet 1 gives you an overview of which condition files (currents and apertures) have been in use recently by which user on which type of resist. On sheet 2 in this logbook you can find a writing time estimation program; please use this prior to requesting e-beam sessions. If in doubt how to use it, contact the e-beam team at [mailto:e-beam@danchip.dtu.dk].
On the L-drive, a logbook for the e-beam writer can be found. Sheet 1 gives you an overview of which condition files (currents and apertures) have been in use recently by which user on which type of resist. On sheet 2 in this logbook you can find a writing time estimation program; please use this prior to requesting e-beam sessions. If in doubt how to use it, contact the e-beam team at [mailto:e-beam@danchip.dtu.dk].


= E-beam resists and Process Flows =
= E-beam resists and Process Flows <span style="font-size: 50%; text-align: right;">[[Specific_Process_Knowledge/Lithography/EBeamLithography#top|top of this page]]</span>=


{|border="1" cellspacing="1" cellpadding="3" style="text-align:left;" width="100%"
{|border="1" cellspacing="1" cellpadding="3" style="text-align:left;" width="100%"