Spin Track 1 + 2 is an SVG 88 series track system from Rite Track. Both tracks have a HMDS priming module, a spin coater, and a hotplate. In fack, the only difference between the two tracks is the resist used in the spin coating. Spin Track 1 + 2 is capable of handling 150 mm wafers, as well as 100 mm wafets, but is currently set up for 100 mm wafer processing. | Spin Track 1 + 2 is an SVG 88 series track system from Rite Track. Both tracks have a HMDS priming module, a spin coater, and a hotplate. In fack, the only difference between the two tracks is the resist used in the spin coating. Spin Track 1 + 2 is capable of handling 150 mm wafers, as well as 100 mm wafets, but is currently set up for 100 mm wafer processing. | ||
'''The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager | '''The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=313 LabManager]''' | ||
<!-- remember to remove the type of documents that are not present --> | <!-- remember to remove the type of documents that are not present --> | ||
===Process information=== | |||
=== Process information === | |||
Link to process pages - e.g. one page for each material | Link to process pages - e.g. one page for each material | ||
Revision as of 13:29, 12 June 2013
Coaters: Comparison Table
| Equipment | SSE Spinner | KS Spinner | |
|---|---|---|---|
| Purpose |
|
| |
| Performance | Substrate handling |
|
|
| Permanent media |
|
| |
| Manual dispense option |
|
| |
| Process parameter range | Parameter 1 |
|
|
| Parameter 2 |
|
| |
| Substrates | Batch size |
|
|
| Allowed materials |
|
| |
SSE Spinner

The SSE spinner MAXIMUS: positioned in Cleanroom 13.
SSE Spinner, Maximus 804, SSE Sister Semiconductor Equipment is a resist spinning system at Danchip which can be used for spinning on 2", 4" and 6" substrates.
The system is equipped with 2 different resists lines:
- AZ5214E and
- AZ4562 and
- 2 syringe lines, which can be used for spinning of e-beam resist.
The user manual(s), quality control procedure(s) and results and contact information can be found in LabManager: Equipment info in LabManager
A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here.
Spin Track 1 + 2

Feedback to this page: click here
Spin Track 1 + 2 is an SVG 88 series track system from Rite Track. Both tracks have a HMDS priming module, a spin coater, and a hotplate. In fack, the only difference between the two tracks is the resist used in the spin coating. Spin Track 1 + 2 is capable of handling 150 mm wafers, as well as 100 mm wafets, but is currently set up for 100 mm wafer processing.
The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager
Process information
Link to process pages - e.g. one page for each material
Example:
- Etch of silicon using RIE
- Etch of silicon oxide using RIE
- Etch of silicon nitride using RIE
- Etch of photo resist using RIE
| Equipment | Equipment 1 | Equipment 2 | |
|---|---|---|---|
| Purpose |
|
| |
| Performance | Response 1 |
|
|
| Response 2 |
|
| |
| Process parameter range | Parameter 1 |
|
|
| Parameter 2 |
|
| |
| Substrates | Batch size |
|
|
| Allowed materials |
|
| |
KS Spinner
A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here.
A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here.
A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here.
Manual Spinner 1 (Laurell)

A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here.
A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here.