| Line 5: | Line 5: | ||
[[Image:fumehoodetch-gold.jpg |300x300px|thumb|Wet Gold Etch: Done in the fumehood positioned in cleanroom 2]] | [[Image:fumehoodetch-gold.jpg |300x300px|thumb|Wet Gold Etch: Done in the fumehood positioned in cleanroom 2]] | ||
Etching of Gold is done wet at Danchip making your own set up in a beaker in the fumehood. You can see the APV [http://www.labmanager.danchip.dtu.dk/d4Show.php?id=2479&mach=146 here]. | Etching of Gold is done wet at Danchip making your own set up in a beaker in the fumehood. You can see the APV [http://www.labmanager.danchip.dtu.dk/d4Show.php?id=2479&mach=146 here]. | ||
We have two different solutions: | We have two different solutions: | ||