| Line 76: | Line 76: | ||
|20HF 6s | |20HF 6s | ||
20LF 2s | 20LF 2s | ||
|Low stress nitride - standard recipe | |Low stress nitride - standard recipe. The latest measured values can be seen in the process control sheet in LabManager. | ||
|- | |- | ||
|LFSiN | |LFSiN | ||