The "SiO<sub>2</sub> target (RF sputter)" study was done on clean Si substrates. The sputter power was 157W and the pressure 3.5 mTorr using RF sputtering of a SiO<sub>2</sub> target. The film thicknesses were around 42 nm.
The "SiO<sub>2</sub> target (RF sputter)" study was done on clean Si substrates. The sputter power was 157W and the pressure 3.5 mTorr using RF sputtering of a SiO<sub>2</sub> target. The film thicknesses were around 42 nm.


===From SiO<sub>2</sub> target (RF sputter)===
====From SiO<sub>2</sub> target (RF sputter)====