Specific Process Knowledge/Thin film deposition/Cluster-based multi-chamber high vacuum sputtering deposition system: Difference between revisions
Appearance
| Line 235: | Line 235: | ||
Bla bla | Bla bla | ||
<gallery caption="Deposition rates of HfO2 at different temperaturs. ALD window." widths="600px" heights=" | <gallery caption="Deposition rates of HfO2 at different temperaturs. ALD window." widths="600px" heights="4 | ||
00px" perrow="2"> | |||
image:Kaempe_Lesker_Load_Loak_image1.png| Deposition rate of HfO<sub>2</sub> at 150 <sup>o</sup>C. Substrate: Silicon 6" wafer with native oxide. | image:Kaempe_Lesker_Load_Loak_image1.png| Deposition rate of HfO<sub>2</sub> at 150 <sup>o</sup>C. Substrate: Silicon 6" wafer with native oxide. | ||
image:Kaempe_Lesker_Load_Loak_image2.png| Deposition rate of HfO<sub>2</sub> at 150 <sup>o</sup>C. Substrate: Silicon 6" wafer with native oxide. | image:Kaempe_Lesker_Load_Loak_image2.png| Deposition rate of HfO<sub>2</sub> at 150 <sup>o</sup>C. Substrate: Silicon 6" wafer with native oxide. | ||