LabAdviser/Technology Research/Nanoscale characterization of ultra-thin metal films for nanofabrication applications: Difference between revisions
Appearance
| Line 8: | Line 8: | ||
==Project Description== | ==Project Description== | ||
The aim of this | The aim of this project is to obtain a deeper understanding of the interaction at the nanoscale level between ultra-thin metal films used in micro/nanofabrication, exploiting the unique capabilities of thin-film fabrication and characterization offered by the combination of the DTU Danchip/Cen facilities. | ||
With the constant miniaturization of the devices and the fabrication of increasingly complex multi-material structures, the interaction between different ultra-thin layers has gained considerable importance in the field of thin-film science and technology in recent years. Therefore the characterization of such interactions in a wide range of temperatures and the description of their impact on the chemical composition, morphology and distribution of crystallographic orientations of multilayer thin-films is of utmost importance. | With the constant miniaturization of the devices and the fabrication of increasingly complex multi-material structures, the interaction between different ultra-thin layers has gained considerable importance in the field of thin-film science and technology in recent years. Therefore the characterization of such interactions in a wide range of temperatures and the description of their impact on the chemical composition, morphology and distribution of crystallographic orientations of multilayer thin-films is of utmost importance. | ||
The project focuses in particular on the description of the interaction between noble metal films, widely used in different areas of micro- and nanofabrication, and extremely thin films of reactive transition metals, used to enhance adhesion onto the substrate - and thus referred as | The project focuses in particular on the description of the interaction between noble metal films, widely used in different areas of micro- and nanofabrication, and extremely thin films of reactive transition metals, used to enhance adhesion onto the substrate - and thus referred as "adhesion layers". Different material and multilayer combinations are investigated; particular emphasis is placed on the description and use of the recently developed transmission Kikuchi diffraction technique for the in-situ study of thin-film nanostructure evolution with changing chemical composition and temperature. | ||
==Transmission Kikuchi diffraction== | ==Transmission Kikuchi diffraction== | ||