Specific Process Knowledge/Thin film deposition/Deposition of Silicon Nitride/Deposition of Silicon Nitride using PECVD: Difference between revisions
Appearance
| Line 133: | Line 133: | ||
|- | |- | ||
|Refractive Index | |Refractive Index | ||
| | |2.02 - 2.04 | ||
|} | |} | ||
|- | |- | ||