'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/PECVD click here]''' <br> | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/PECVD click here]''' <br> | ||
==PECVD Plasma Enhanced Chemical Vapor Deposition== | ==PECVD Plasma Enhanced Chemical Vapor Deposition== | ||
| Line 110: | Line 108: | ||
*Ar:0-1415 sccm | *Ar:0-1415 sccm | ||
*5%PH<sub>3</sub>:0-100 sccm | *5%PH<sub>3</sub>:0-100 sccm | ||
*3%B<sub>2</sub>H<sub>6</sub>:0- | *3%B<sub>2</sub>H<sub>6</sub>:0-270 sccm | ||
|- | |- | ||
!style="background:silver; color:black" align="left" rowspan="3" valign="top" |Substrates | !style="background:silver; color:black" align="left" rowspan="3" valign="top" |Substrates | ||