Specific Process Knowledge/Characterization/Optical microscope: Difference between revisions

From LabAdviser
Jbram (talk | contribs)
No edit summary
Jbram (talk | contribs)
No edit summary
 
Line 10: Line 10:
|-style="background:white; color:black; vertical-align:middle; text-align:center;"
|-style="background:white; color:black; vertical-align:middle; text-align:center;"
|
|
!Nikon<br>SMZ 1000
 
!Noco IR
!Noco IR
!Leica<br>INM 100
!Leica<br>INM 100
Line 27: Line 27:
|-style="background:white; color:black; vertical-align:middle; text-align:center;"
|-style="background:white; color:black; vertical-align:middle; text-align:center;"
|
|
|[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|[[image:Noco IR microscope.jpg|100x100px|thumb|center]][[image:Noco IR microscope_1.jpg|100x100px|thumb|center]]
|[[image:Noco IR microscope.jpg|100x100px|thumb|center]][[image:Noco IR microscope_1.jpg|100x100px|thumb|center]]
|[[image:LeicaINM100.jpg|100x100px|thumb|center]]
|[[image:LeicaINM100.jpg|100x100px|thumb|center]]
Line 44: Line 43:
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;"
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;"
!Location
!Location
|346-901
|346-901
|346-901
|346-901
|346-901
|cleanroom<br>D-3
|cleanroom<br>D-3?
|cleanroom<br>D-3
|cleanroom<br>D-3
|cleanroom<br>A-1
|cleanroom<br>A-1
Line 61: Line 60:
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;"
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;"
!Responsible<br>group
!Responsible<br>group
|Wet chemistry
|Wet chemistry
|Wet chemistry
|Wet chemistry
|Wet chemistry
Line 78: Line 76:
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;"
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;"
!Objectives
!Objectives
|Zoom 0.8x - 8x
|
|
*2.5x
*2.5x
Line 147: Line 144:
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;"
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;"
!Ocular
!Ocular
|10x
|10x
|10x
|10x
|10x
Line 164: Line 160:
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;"
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;"
!Special<br>features
!Special<br>features
|Stereoscopic
|IR imaging
|IR imaging
|
|
Line 186: Line 181:
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;"
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;"
!Contrast<br>mechanisms
!Contrast<br>mechanisms
|
*Brightfield
|
|
*Polarizer
*Polarizer
Line 229: Line 222:
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;"
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;"
!Illumination<br>modes
!Illumination<br>modes
|
*Episcopic
|
|
*Episcopic
*Episcopic
Line 267: Line 258:
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;"
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;"
!Camera
!Camera
|None
|IR camera
|IR camera
|DS-Fi2
|DS-Fi2
Line 290: Line 280:
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;"
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;"
!Analysis<br>software
!Analysis<br>software
|None
|None
|None
|NIS-D
|NIS-D

Latest revision as of 09:52, 1 April 2026

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

Noco IR Leica
INM 100
Zeiss
Jenatech
Nikon Eclipse
L200 #1
Nikon Eclipse
L200 #2
Nikon Eclipse
L200N #3
Nikon Eclipse
L200N #4
Nikon
ME 600
Leica
S8 APO
Zeiss
Axiotron
Olympus
MX63
Location 346-901 346-901 cleanroom
D-3
cleanroom
D-3
cleanroom
A-1
cleanroom
D-3
cleanroom
E-5
cleanroom
F-1
cleanroom
Cx1
cleanroom
F-3
cleanroom
E-4
Responsible
group
Wet chemistry Wet chemistry Lithography Lithography Lithography Lithography Lithography Lithography Lithography Lithography Lithography
Objectives
  • 2.5x
  • 10x
  • 20x
  • 50x
  • 2.5x
  • 5x
  • 10x
  • 20x
  • 50x
  • 5x
  • 10x
  • 20x
  • 50x
  • 100x
  • 2.5x
  • 5x
  • 10x
  • 20x
  • 50x
  • 2.5x
  • 5x
  • 10x
  • 20x
  • 50x
  • 100x
  • 2.5x
  • 5x
  • 10x
  • 20x
  • 50x
  • 100x
  • 2.5x
  • 5x
  • 10x
  • 20x
  • 50x
  • 100x
  • 5x
  • 10x
  • 20x
  • 50x
  • 100x
Zoom 1x - 8x
  • 5x
  • 10x
  • 20x
  • 50x
  • 1.25x
  • 5xBD
  • 10xBD
  • 20xBD
  • 50xBD
  • 100xBD
Ocular 10x 10x 10x 10x 10x 10x 10x 10x 10x 10x 10x
Special
features
IR imaging


Stereoscopic
Contrast
mechanisms
  • Polarizer
  • Brightfield
  • Brightfield
  • Darkfield
  • Polarizer
  • Brightfield
  • Brightfield
  • Darkfield
  • Brightfield
  • Darkfield
  • Polarizer
  • Brightfield
  • Darkfield
  • Polarizer
  • Brightfield
  • Darkfield
  • Polarizer
  • Brightfield
  • Darkfield
  • Brightfield
  • Brightfield
  • Darkfield
  • Polarizer
  • Brightfield
  • Darkfield
Illumination
modes
  • Episcopic
  • Diascopic
  • Episcopic
  • Diascopic
  • Episcopic
  • Diascopic
  • Episcopic
  • Diascopic
  • Episcopic
  • Diascopic
  • Episcopic
  • Diascopic
  • Episcopic
  • Diascopic
  • Episcopic
  • Episcopic
  • Episcopic
  • Diascopic
  • Episcopic
  • Diascopic
Camera IR camera DS-Fi2 None DS-Fi1 DS-Fi1
  • DS-Fi2
  • C-mount,
    0.7x relay
  • DS-Fi2
  • C-mount,
    0.7x relay
DS-Fi2 None Infinity X
  • DP23-CU
  • C-mount
Analysis
software
None NIS-D None NIS-BR NIS-D NIS-D NIS-D NIS-D None DeltaPix PRECiV Core


There are also two optical microscopes in building 451, a stereo microscope and a transmission microscope, that were both previously located in Packlab. Please ask staff / the BioMic group for details.