==Anneal-bond furnace (C3)== | ==Anneal-bond furnace (C3)== | ||
| Line 76: | Line 76: | ||
*Wafers and samples from PECVD4 | *Wafers and samples from PECVD4 | ||
*Wafers and samples from PECVD3 (without any metals) | *Wafers and samples from PECVD3 (without any metals) | ||
*Wafers from Wafer Bonder | *Wafers from Wafer Bonder 02 | ||
*Wafers from Wafer Bonder | *Wafers from Wafer Bonder 03 (without any metals). Use new or dedicated/clean teflon sheets in the wafer bonder | ||
|- | |- | ||
|} | |} | ||