*Dry oxide: ~ 0 nm to 300 nm (it takes too long to grow thicker dry oxide layers) | *Dry oxide: ~ 0 nm to 300 nm (it takes too long to grow thicker dry oxide layers) | ||
*Wet oxide: ~ 0 nm to 3 µm (~23 hours wet oxidation at 1100 <sup>o</sup>C) | *Wet oxide: ~ 0 nm to 3 µm (~23 hours wet oxidation at 1100 <sup>o</sup>C) | ||