Specific Process Knowledge/Thin film deposition/Deposition of Hafnium Oxide: Difference between revisions
Appearance
| (2 intermediate revisions by the same user not shown) | |||
| Line 5: | Line 5: | ||
<br clear="all" /> | <br clear="all" /> | ||
=Hafnium oxide (HfO₂)= | =Hafnium oxide (HfO₂)= | ||
| Line 19: | Line 17: | ||
Thin films of hafnium oxide, HfO<sub>2</sub>, can be deposited both in the [[Specific Process Knowledge/Thin film deposition/ALD Picosun R200|ALD1]] and the [[Specific Process Knowledge/Thin film deposition/ALD2 (PEALD)|ALD2 (PEALD)]]. However, it is preferred to use the ALD1. | Thin films of hafnium oxide, HfO<sub>2</sub>, can be deposited both in the [[Specific Process Knowledge/Thin film deposition/ALD Picosun R200|ALD1]] and the [[Specific Process Knowledge/Thin film deposition/ALD2 (PEALD)|ALD2 (PEALD)]]. However, it is preferred to use the ALD1. | ||
More information about hafnium oxide deposition can be found here: | More information about hafnium oxide deposition can be found here: | ||
*[[Specific_Process_Knowledge/Thin_film_deposition/ALD_Picosun_R200/HfO2_deposition_using_ALD_new_page|ALD deposition of HfO<sub>2</sub> in ALD1]] | |||
*[[Specific Process Knowledge/Thin film deposition/ALD2 (PEALD)/HfO2 deposition using ALD2|ALD deposition of HfO<sub>2</sub> in ALD2]]. | |||
==Deposition of hafnium oxide== | ==Deposition of hafnium oxide== | ||