Specific Process Knowledge/Thin film deposition/Deposition of NiV: Difference between revisions
Appearance
| (One intermediate revision by the same user not shown) | |||
| Line 3: | Line 3: | ||
==Sputtering of Nickel Vanadium== | ==Sputtering of Nickel Vanadium== | ||
Nickel Vanadium may be sputter deposited in the Sputter-system (Lesker) and the Sputter-system Metal-Oxide. The following pages show both process parameters and data on surface roughness of the deposited films: | Nickel Vanadium may be sputter deposited in the Sputter-system (Lesker) and the Sputter-system Metal-Oxide (PC1). The following pages show both process parameters and data on surface roughness of the deposited films: | ||
* [[/Sputtering of NiV in Lesker|Sputtering of NiV in Lesker]] | * [[/Sputtering of NiV in Lesker|Sputtering of NiV in Sputter-System (Lesker)]] | ||
* [[/Sputtering of NiV in Sputter-System Metal-Oxide (PC1)|Sputtering of NiV in Sputter-System Metal-Oxide (PC1)]] | * [[/Sputtering of NiV in Sputter-System Metal-Oxide (PC1)|Sputtering of NiV in Sputter-System Metal-Oxide (PC1)]] | ||
* [[/Sputtering of NiV in Wordentec|Sputtering of NiV in Wordentec]] (tool now decommissioned, but results | * [[/Sputtering of NiV in Wordentec|Sputtering of NiV in Wordentec]] (tool now decommissioned, but results are of general interest) | ||
Latest revision as of 11:11, 18 July 2025
Feedback to this page: click here
Sputtering of Nickel Vanadium
Nickel Vanadium may be sputter deposited in the Sputter-system (Lesker) and the Sputter-system Metal-Oxide (PC1). The following pages show both process parameters and data on surface roughness of the deposited films:
- Sputtering of NiV in Sputter-System (Lesker)
- Sputtering of NiV in Sputter-System Metal-Oxide (PC1)
- Sputtering of NiV in Wordentec (tool now decommissioned, but results are of general interest)
In the chart below you can compare the available sputter systems:
| Sputter deposition (Sputter-System Lesker) | Sputter deposition (Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3)) | |
| General description | Sputter deposition of NiV | Sputter deposition of NiV |
| Pre-clean | none | RF Ar clean |
| Layer thickness | About 10Å to 5000Å | About 10Å to 5000Å |
| Deposition rate | Depending on process parameters(normally less than 1 Å/s). | Depending on process parameters(normally less than 1 Å/s). |
| Batch size |
|
|
| Allowed substrates |
|
|
| Allowed materials |
|
|
| Target size | 2 inch sputter target | 3 inch sputter target
(or in special cases 4 inch) |
| Comment |
|
|