Specific Process Knowledge/Characterization/Sensofar S Neox: Difference between revisions
Appearance
Created page with "{{cc-nanolab}} '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Sensofar S Neox click here]''' Characterization Profiler Profiler ==Optical Profiler (Sensofar S Neox) == {{CC-bghe2}} image:IMG_4555.JPG|275x275px|right|thumb|Optical Profiler (Sensofar): positioned in the clea..." |
|||
| (9 intermediate revisions by the same user not shown) | |||
| Line 1: | Line 1: | ||
{{cc-nanolab}} | {{cc-nanolab}} | ||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Sensofar_S_Neox click here]''' | ||
<br> | |||
[[Category:Equipment|Characterization Profiler]] | [[Category:Equipment|Characterization Profiler]] | ||
[[Category:Characterization|Profiler]] | [[Category:Characterization|Profiler]] | ||
<br> | |||
= | = Sensofar S Neox (Optical Profiler) = | ||
{{CC-bghe2}} | {{CC-bghe2}} | ||
[[image:IMG_4555.JPG|275x275px|right|thumb|Optical Profiler (Sensofar): positioned in the clean room C-1), {{photo1}}]] | [[image:IMG_4555.JPG|275x275px|right|thumb|Optical Profiler (Sensofar): positioned in the clean room C-1), {{photo1}}]] | ||
| Line 23: | Line 23: | ||
'''Analysis software:''' | '''Analysis software:''' | ||
*Free analysis software for visualizing and analyzing AFM and Optical profiler files (Sensofar) [http://gwyddion.net Gwyddion] | *Free analysis software for visualizing and analyzing AFM and Optical profiler files (Sensofar) [http://gwyddion.net Gwyddion] | ||
*SensoView software from | *SensoView software from Sensofar can be downloaded from the cleanroom drive : <br> | ||
:\CleanroomDrive\_Equipment\Optical profiler Sensofar\ | |||
*We have an extra license to the more advanced SensoMap software. It can be accessed by Remote Desktop: '''DTU-8CC0321MFL''' (''log-in using your DTU credentials''). | |||
[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=491 | The user manual, technical information (SensoSCAN and SensoVIEW manuals) and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=491 LabManager]. | ||
| Line 37: | Line 37: | ||
*[https://labmanager.dtu.dk/view_binary.php?fileId=5346|S Neox leaflet including specifications] - requires login | *[https://labmanager.dtu.dk/view_binary.php?fileId=5346|S Neox leaflet including specifications] - requires login | ||
*Acceptance measurements on the S Neox Sensofar: [[Media:Acceptance measurements on Nanolab samples.pdf]], measured at the acceptances test by Sensofar and Berit Herstrøm@ DTU Nanolab | *Acceptance measurements on the S Neox Sensofar: [[Media:Acceptance measurements on Nanolab samples.pdf]], measured at the acceptances test by Sensofar and Berit Herstrøm@ DTU Nanolab | ||
* | *[//Optical_Profiler_(Sensofar)_acceptance_test Results from the Optical Profiler (Sensofar) acceptance test - for the previous system - expired!!] | ||
<br> | |||
=== | ===Performance and Process Parameters=== | ||
{| border="2" cellspacing="0" cellpadding="10" | {| border="2" cellspacing="0" cellpadding="10" | ||