Line 10: Line 10:




==Comparison of Titanium Oxide (ALD) etch Methods [[Image:section under construction.jpg|70px]]==
==Comparison of Titanium Oxide (ALD) etch Methods ==


{|border="1" cellspacing="1" cellpadding="3" style="text-align:left;"  
{|border="1" cellspacing="1" cellpadding="3" style="text-align:left;"  
Line 26: Line 26:
!Generel description
!Generel description
|Wet etch of TiO2 (ALD)
|Wet etch of TiO2 (ALD)
|
|Dry etch of TiO2
|-
|-


Line 34: Line 34:
|2,5 nm/min
|2,5 nm/min
|
|
*~30nm/min (pure Al)
*It has not been explored
*current recipe ~8 nm/min
|-
|-


Line 43: Line 44:
*Isotropic
*Isotropic
|
|
*Isotropic
*Anisotropic
|-
|-


Line 54: Line 55:
*Any size (in beaker)
*Any size (in beaker)
|
|
*Chips (6-60 mm)
*Samples < 150 mm wafers on carrier
*100 mm wafers  
*one 150 mm wafer at a time
*150 mm wafers
|-
|-


Line 65: Line 65:
*Any material
*Any material
|
|
*Every thing that is allowed in the Developer: TMAH Manual
*silicon, silicon oxides and nitrides
*Al, Cr, Ti (incl. oxides and nitrides)
*Ta, W, Nb (incl. oxides and nitrides)
|-
|-
|}
|}

Latest revision as of 15:23, 4 September 2025

Feedback to this page: click here


Etch of Titanium oxide has been test in the ICP metal etcher.


Comparison of Titanium Oxide (ALD) etch Methods

BHF ICP Metal Etcher
Generel description Wet etch of TiO2 (ALD) Dry etch of TiO2
Etch rate range 2,5 nm/min
  • It has not been explored
  • current recipe ~8 nm/min
Etch profile
  • Isotropic
  • Anisotropic
Substrate size
  • Any size (in beaker)
  • Samples < 150 mm wafers on carrier
  • one 150 mm wafer at a time
Allowed materials In beaker:
  • Any material
  • silicon, silicon oxides and nitrides
  • Al, Cr, Ti (incl. oxides and nitrides)
  • Ta, W, Nb (incl. oxides and nitrides)