'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Polymer_Processing click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Polymer_Processing click here]''' | ||
<BR> | <BR> | ||
<BR> | <BR><span style="background:#FF2800">'''THIS PAGE IS UNDER CONSTRUCTION'''</span> | ||
= Polymer Processing = | |||
There is a wide range of methods available to structure and modify polymers, though commonly done outside of a cleanroom. | |||
Many polymer processing methods may require a mask or stamp or some kind, f.ex. injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, f.ex. laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerization are called additive methods as they create the structure by a building up the polymer structure. | Many polymer processing methods may require a mask or stamp or some kind, f.ex. injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, f.ex. laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerization are called additive methods as they create the structure by a building up the polymer structure. | ||
<br> | <br> | ||
| Line 16: | Line 15: | ||
* [[Specific Process Knowledge/Lithography/NanoImprintLithography|Nano Imprint Lithography]] | * [[Specific Process Knowledge/Lithography/NanoImprintLithography|Nano Imprint Lithography]] | ||
* [[Specific_Process_Knowledge/Back-end_processing/Hot_Embosser|Hot Embossing]] (Compression Molding) | * [[Specific_Process_Knowledge/Back-end_processing/Hot_Embosser|Hot Embossing]] (Compression Molding) | ||
* [[Specific Process Knowledge/Back-end processing/Polymer Injection Molder|Polymer Injection Molding]] '' | * [[Specific Process Knowledge/Back-end processing/Polymer Injection Molder|Polymer Injection Molding]] ''(moved to DTU Construct))'' | ||
* Polymer Casting (e.g. PDMS) | * Polymer Casting (e.g. [[Specific Process Knowledge/Characterization/Sample preparation| PDMS Casting]]) | ||
''' | '''Specialized Processes:''' | ||
* UV Lithography | * [[Specific Process Knowledge/Lithography/UVLithography|UV Lithography]] | ||
* Additive Techniques | * Additive Techniques | ||
:* 3D printing | :* 3D printing | ||
:* 2-Photon Polymerization Lithography | :* 2-Photon Polymerization Lithography | ||
* Plasma Etching | * Plasma Etching | ||
* FDTS coating (MVD) | * [[Specific Process Knowledge/Thin film deposition/MVD|FDTS coating (MVD)]] | ||
* Laser Ablation | * [[Specific Process Knowledge/Back-end processing/Laser Micromachining Tool|Laser Ablation/Milling]] | ||
* Micro Milling ''(not generally availabe at DTU Nanolab)'' | * Micro Milling ''(not generally availabe at DTU Nanolab)'' | ||
* Extrusion Coating ''(not availabe at DTU Nanolab)'' | * Extrusion Coating ''(not availabe at DTU Nanolab)'' | ||
<br> | <br> | ||
== Choose Material for Polymer Processing== | == Choose Material for Polymer Processing== | ||
* Epoxy, e.g. SU-8 | * Epoxy, e.g. SU-8 | ||
* Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc | * Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc | ||
* Photo Resist, e.g. AZ resists | * Photo Resist, e.g. AZ resists | ||
Latest revision as of 16:56, 26 November 2025
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
THIS PAGE IS UNDER CONSTRUCTION
Polymer Processing
There is a wide range of methods available to structure and modify polymers, though commonly done outside of a cleanroom.
Many polymer processing methods may require a mask or stamp or some kind, f.ex. injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, f.ex. laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerization are called additive methods as they create the structure by a building up the polymer structure.
Choose Method of Polymer Processing
- Nano Imprint Lithography
- Hot Embossing (Compression Molding)
- Polymer Injection Molding (moved to DTU Construct))
- Polymer Casting (e.g. PDMS Casting)
Specialized Processes:
- UV Lithography
- Additive Techniques
- 3D printing
- 2-Photon Polymerization Lithography
- Plasma Etching
- FDTS coating (MVD)
- Laser Ablation/Milling
- Micro Milling (not generally availabe at DTU Nanolab)
- Extrusion Coating (not availabe at DTU Nanolab)
Choose Material for Polymer Processing
- Epoxy, e.g. SU-8
- Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc
- Photo Resist, e.g. AZ resists