Specific Process Knowledge/Pattern Design: Difference between revisions
Appearance
Tags: Mobile edit Mobile web edit |
|||
| (14 intermediate revisions by 3 users not shown) | |||
| Line 9: | Line 9: | ||
* CleWin | * CleWin | ||
* KLayout (free) | * KLayout (free) link: https://www.klayout.de/ | ||
* L-Edit | * L-Edit | ||
* Autocad | * Autocad | ||
At Nanolab we offer all users '''free access to CleWin 6''' for their mask layout. You can find more information on how to | At Nanolab we offer all users '''free access to CleWin 6''' for their mask layout. You can find more information on how to install CleWin 6 on your local computer [[Specific Process Knowledge/Pattern Design/CleWin|'''here''']]. | ||
<BR> | <BR> | ||
<BR> | <BR> | ||
| Line 21: | Line 21: | ||
* For '''DUV-lithography''', a physical mask, called "reticles", is required. The file format must be GDS. For more details concerning the design of reticles see [[Specific_Process_Knowledge/Lithography/DUVStepperLithography/Reticle_Design|Reticle Design]]. | * For '''DUV-lithography''', a physical mask, called "reticles", is required. The file format must be GDS. For more details concerning the design of reticles see [[Specific_Process_Knowledge/Lithography/DUVStepperLithography/Reticle_Design|Reticle Design]]. | ||
* For '''E-beam lithography''', you need to prepare a set of files (GDS, V30, sdf, jdf and mgn files). For more details, please see [[Specific_Process_Knowledge/Lithography/EBeamLithography/FilePreparation#FilePreparation|File preparation]]. For details about how to make aligned E-beam patterns, please have at look at [[Specific_Process_Knowledge/Lithography/EBeamLithography/JBX9500Manual#Design_of_global_marks_and_chip_marks|Design of global marks and chip marks]] | * For '''E-beam lithography''', you need to prepare a set of files (GDS, V30, sdf, jdf and mgn files). For more details, please see [[Specific_Process_Knowledge/Lithography/EBeamLithography/FilePreparation#FilePreparation|File preparation]]. For details about how to make aligned E-beam patterns, please have at look at [[Specific_Process_Knowledge/Lithography/EBeamLithography/JBX9500Manual#Design_of_global_marks_and_chip_marks|Design of global marks and chip marks]] | ||
* For '''Laser Cutting''' using our [Specific Process Knowledge/Back-end processing/Laser Micromachining Tool|Laser Micromachining Tool], the layout file must be saved as DXF file. | * For '''Laser Cutting''' using our [[Specific Process Knowledge/Back-end processing/Laser Micromachining Tool|Laser Micromachining Tool]], the layout file must be saved as DXF file. | ||
<br> | <br> | ||
<br> | <br> | ||
| Line 38: | Line 38: | ||
*Maskless aligner: | *Maskless aligner: | ||
**[[Media:MLA AlignmentMarks simple.gds|Simple alignment marks (.gds)]] | **[[Media:MLA AlignmentMarks simple.gds|Simple alignment marks (.gds)]] | ||
**[[Media: | **[[Media:MLA_alignmentMarks_arrows.cif|Alignment marks with structures to assist in locating the marks during alignment (.cif)]] | ||
**[[Media: | **[[Media:AlignmentMark_KOH.cif|Alignment mark for multiple layers, Layer 1 for etch in KOH (.cif)]] | ||
<br> | <br> | ||
===Alignment marks location=== | ===Alignment marks location=== | ||
For the mask aligners [[Specific_Process_Knowledge/Lithography/UVExposure#Aligner:_MA6-1|MA6-1]] and [[Specific_Process_Knowledge/Lithography/UVExposure#Aligner:_MA6-2|MA6-2]] | For the mask aligners [[Specific_Process_Knowledge/Lithography/UVExposure#Aligner:_MA6-1|MA6-1]] and [[Specific_Process_Knowledge/Lithography/UVExposure#Aligner:_MA6-2|MA6-2]] | ||
* | *For Top Side Alignment (TSA) alignment marks should be located 35-80 mm in left and right in horizontal location (X) from mask center and between -20 and +20 mm in vertical location (Y) | ||
*For Back Side Alignment (BSA) alignment marks should be located 15-45 mm in left and right in horizontal location (X) from mask center and between -20 and +20 mm in vertical location (Y) | |||
<br> | <br> | ||
=== Alignment marks for E-beam lithography === | === Alignment marks for E-beam lithography === | ||
If your UV mask is used to define wafers marks in e-beam lithography with JEOL JBX-9500, you should design your alignment marks in a way the JEOL JBX-9500 recognizes. Please follow the guide [ | If your UV mask is used to define wafers marks in e-beam lithography with JEOL JBX-9500, you should design your alignment marks in a way the JEOL JBX-9500 recognizes. Please follow the guide [[Specific_Process_Knowledge/Lithography/EBeamLithography/JEOLAlignment|to e-beam alignment here]] | ||
<br> | <br> | ||
<br> | <br> | ||
=== Helpful information for chip layout === | === Helpful information for chip layout === | ||
*[[Media:Gamma coater & developer chucks + hotplate pins.gds|Gamma coater & developer chucks + hotplate pins.gds]] Design file showing the size of the chucks and the position of the hotplate pins in the Gamma tools. | *[[Media:Gamma coater & developer chucks + hotplate pins.gds|Gamma coater & developer chucks + hotplate pins.gds]] Design file showing the size of the chucks and the position of the hotplate pins in the Gamma tools. | ||
| Line 62: | Line 59: | ||
== Mask Ordering and Fabrication == | == Mask Ordering and Fabrication == | ||
Our standard mask supplier is [https://www.macdermidalpha.com/semiconductor-solutions/compugraphics Compugraphics]. They can provide 5" and 7" masks on soda lime glass or quartz. Minimum feature size can be 0.8µm, 1µm or 1.5µm which is reflected in the price. Read a short guide on[[Media:Mask Ordering Guide.pdf| how to order photomasks from Compugraphics]] here. Templates for the mask specifications for 5" and 7" masks respectively can be seen [[ | Our standard mask supplier is [https://www.macdermidalpha.com/semiconductor-solutions/compugraphics Compugraphics]. They can provide 5" and 7" masks on soda lime glass or quartz. Minimum feature size can be 0.8µm, 1µm or 1.5µm which is reflected in the price. Read a short guide on[[Media:Mask Ordering Guide.pdf| how to order photomasks from Compugraphics]] here. Templates for the mask specifications for 5" and 7" masks respectively can be seen [[/Mask Specifications| <b>here</b>.]] | ||
The masks have to be ordered in Procure. Nanolab cannot order the mask for you but we do offer a final check of the design and mask specifications before you place the order. You can find a guide on [[Media:Maskordering in Fusion.pdf| how to order and attach design files in procure]] here. | The masks have to be ordered in Procure. Nanolab cannot order the mask for you but we do offer a final check of the design and mask specifications before you place the order. You can find a guide on [[Media:Maskordering in Fusion.pdf| how to order and attach design files in procure]] here. | ||
| Line 71: | Line 68: | ||
Give each layer appropriate GDS number respectively CIF names before exporting the file. This is done by double click on the layers and fill out the window that pops up. | Give each layer appropriate GDS number respectively CIF names before exporting the file. This is done by double click on the layers and fill out the window that pops up. | ||
We can also provide guidance regarding the mask design phase. Please contact the | We can also provide guidance regarding the mask design phase. Please contact the [mailto:nanolabsupport@nanolab.dtu.dk | Fabrication Support Team] for help and review. | ||
*[[Media:Maskordering in Fusion.pdf| How to order and attach design files in DTU Fusion]] | *[[Media:Maskordering in Fusion.pdf| How to order and attach design files in DTU Fusion]] | ||
*[[ | *[[/Mask Specifications| Templates for 5" and 7" Mask Specifications]] | ||