Specific Process Knowledge/Etch/Etching of Molybdenum: Difference between revisions
Appearance
No edit summary |
|||
| (2 intermediate revisions by 2 users not shown) | |||
| Line 1: | Line 1: | ||
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.''' | '''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.''' | ||
'''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.''' | '''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.''' | ||
'''Feedback to this page''': '''[mailto:labadviser@ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Molybdenum click here]''' | ||
Latest revision as of 15:43, 28 March 2025
Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.
All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.
Feedback to this page: click here
Comparison of Molybdenum Etch Methods
| Mo wet etch | Dry etch | |
|---|---|---|
| Generel description | Wet etch of Mo using Chrome etch 18 | Dry etch of Mo |
| Etch rate range |
|
|
| Etch profile |
|
|
| Masking material |
|
|
| Substrate size |
|
|
| Allowed materials |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |