Specific Process Knowledge/Thin film deposition/Deposition of Silicon Oxide/Deposition of Silicon Oxide using LPCVD TEOS: Difference between revisions

Pevo (talk | contribs)
Pevo (talk | contribs)
 
(3 intermediate revisions by the same user not shown)
Line 67: Line 67:
==Deposition rate and refractive index:==
==Deposition rate and refractive index:==


The deposition rate is normally a little below 10 nm/min. But especially for short depositions, the deposition rate is higher and depends on the deposition time. The mean reason for this is that there is some TEOS (about 20-30 nm) will be deposited during the pre- and post-deposition steps, and this does not count as deposition time. The pre-deposition step is when the TEOS is introduced into the furnace tube before the deposition, and the pre-deposition step is when the TEOS gas line and mass flow controller are emptied through the furnace tube after the deposition.  
The deposition rate is normally a little below 10 nm/min - See process log in LabManager. But especially for short depositions, the deposition rate is higher and depends on the deposition time. The main reason for this is that there is some TEOS (about 20-30 nm) being deposited during the pre- and post-deposition steps in the recipe, and this does not count as deposition time. The post-deposition step is when the TEOS is introduced into the furnace tube before the deposition, and the pre-deposition step is when the TEOS gas line and MFC are emptied through the furnace tube after the deposition.  


Before you use the furnace, it is recommended to look at process log to find the latest deposition rates.
Before you use the furnace, it is recommended to look at process log to find the latest deposition rates.
Line 77: Line 77:
==Using LPCVD TEOS oxide as a masking material for KOH etching==
==Using LPCVD TEOS oxide as a masking material for KOH etching==


It is possible to use LPCVD TEOS pxide as a masking layer for KOH etching. However, it is not as suitable as LPCVD silicon nitride for deep KOH etching, as the the etch rate for TEOS oxide is higher than the etch rate for silicon nitride.
It is possible to use LPCVD TEOS oxide as a masking layer for KOH etching. However, it is not as suitable as LPCVD silicon nitride for deep KOH etching, as the etch rate for TEOS oxide is higher than the etch rate for silicon nitride.