Etching of nanostructures in Si using DRIE-Pegasus: nano1.4 recipe, Run ID 2000, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/50 coil/platen, -20 degs. |
uploaded a new version of "Image:WF 2E07a mar23 2011-030.jpg": Etching of nanostructures in Si using DRIE-Pegasus: nano1.4 recipe, Run ID 2000, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/50 coil/platen, -20 degs. |
(No difference)
| |
Latest revision as of 12:42, 29 April 2011
Etching of nanostructures in Si using DRIE-Pegasus: nano1.4 recipe, Run ID 2000, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/50 coil/platen, -20 degs.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 12:42, 29 April 2011 | 1,024 × 768 (133 KB) | Jml (talk | contribs) | Etching of nanostructures in Si using DRIE-Pegasus: nano1.4 recipe, Run ID 2000, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/50 coil/platen, -20 degs. | |
| 12:40, 29 April 2011 | 1,024 × 768 (93 KB) | Jml (talk | contribs) | Etching of nanostructures in Si using DRIE-Pegasus: nano1.4 recipe, Run ID 2000, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/50 coil/platen, -20 degs. |
You cannot overwrite this file.
File usage
The following page uses this file: