Specific Process Knowledge/Lithography/Coaters/Spin Coater: Gamma UV processing: Difference between revisions
Appearance
No edit summary |
|||
| (4 intermediate revisions by 2 users not shown) | |||
| Line 1: | Line 1: | ||
{{ | {{cc-nanolab}} | ||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Lithography/Coaters/Spin_Coater:_Gamma_UV_processing click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Lithography/Coaters/Spin_Coater:_Gamma_UV_processing click here]''' | ||
| Line 54: | Line 54: | ||
|- | |- | ||
| | | | ||
*[ | *[https://labmanager.dtu.dk/d4Show.php?id=5123&mach=359 The QC procedure for Spin Coater: Gamma UV] - '''requires login'''<br> | ||
*[ | *[https://labmanager.dtu.dk/view_binary.php?type=data&mach=359 The newest QC data for Spin Coater: Gamma UV] - '''requires login''' | ||
{| {{table}} | {| {{table}} | ||
| align="center" | | | align="center" | | ||
| Line 109: | Line 109: | ||
|- | |- | ||
| | | | ||
*[ | *[https://labmanager.dtu.dk/d4Show.php?id=5123&mach=359 The QC procedure for Spin Coater: Gamma UV] - '''requires login'''<br> | ||
*[ | *[https://labmanager.dtu.dk/view_binary.php?type=data&mach=359 The newest QC data for Spin Coater: Gamma UV] - '''requires login''' | ||
{| {{table}} | {| {{table}} | ||