Created page with "= XRD SmartLab = The Rigaku 9kW Rotating Anode XRD SmartLab is an advanced XRD instrument for measuring thin films, powders, and other substances. All thin films can be measured without fixating the sample, as the system has a so called In-Plane arm. 400x400px|right|thumb|The XRD SmartLab located in a basement 346-904 '''The user manual(s), user APV(s), technical information, and contact information can be found in LabManager:'''..."
 
Mmat (talk | contribs)
mNo edit summary
 
(14 intermediate revisions by 2 users not shown)
Line 1: Line 1:
= XRD SmartLab =
{{cc-nanolab}}


The Rigaku 9kW Rotating Anode XRD SmartLab is an advanced XRD instrument for measuring thin films, powders, and other substances. All thin films can be measured without fixating the sample, as the system has a so called In-Plane arm.
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/XRD/XRD_SmartLab_9kW_Rotating_Anode click here]'''
 
 
= XRD Rot Anode =
 
The Rigaku SmartLab 9kW Rotating Anode XRD that we call "XRD Rot Anode" is an advanced XRD instrument for measuring thin films, powders, and other substances. All thin films can be measured without fixating the sample, as the system has a so called In-Plane arm.


[[image:eves_XRD_RotAnode_01.jpg|400x400px|right|thumb|The XRD SmartLab located in a basement 346-904]]
[[image:eves_XRD_RotAnode_01.jpg|400x400px|right|thumb|The XRD SmartLab located in a basement 346-904]]
Line 11: Line 16:




Various measurement types including X-Ray reflectivity, Rocking curve, Theta-2theta, and Pole figures are described here:
Various measurement types including X-Ray Reflectivity, Rocking Curve, Theta-2theta, and Pole figures are described here:


[http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XRD/Process_Info  Process information]
[http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XRD/Process_Info  Process information]
Line 18: Line 23:
The measurement settings and results of the pre-acceptance test are described in this document, also found on the Lab Manager:
The measurement settings and results of the pre-acceptance test are described in this document, also found on the Lab Manager:


*[https://labmanager.dtu.dk/view_binary.php?fileId=5413| (FAT) Factory Acceptance Test] - requires login
* [https://labmanager.dtu.dk/view_binary.php?class=MiscDocument&id=3&name=FAT_XRD_RotAnode_DTU-RigakuXRD-Report.pdf |(FAT) Factory Acceptance Test  - requires login]


The same measurement were completed as part of the acceptance, but no report was generated. In addition the inspection certificate is available here:  
The same measurement were completed as part of the acceptance, but no report was generated. In addition the inspection certificate is available here:  


*[https://labmanager.dtu.dk/view_binary.php?fileId=5414| (SAT) Site Acceptance Test]  - requires login
* [https://labmanager.dtu.dk/view_binary.php?class=MiscDocument&id=3&name=Inspection_Certificate_XRD_RotAnode_2024.pdf |(SAT) Site Acceptance Test]  - requires login

Latest revision as of 19:26, 10 June 2025

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here


XRD Rot Anode

The Rigaku SmartLab 9kW Rotating Anode XRD that we call "XRD Rot Anode" is an advanced XRD instrument for measuring thin films, powders, and other substances. All thin films can be measured without fixating the sample, as the system has a so called In-Plane arm.

The XRD SmartLab located in a basement 346-904


The user manual(s), user APV(s), technical information, and contact information can be found in LabManager:

XRD RotAnode SmartLab in LabManager - requires login


Various measurement types including X-Ray Reflectivity, Rocking Curve, Theta-2theta, and Pole figures are described here:

Process information


The measurement settings and results of the pre-acceptance test are described in this document, also found on the Lab Manager:

The same measurement were completed as part of the acceptance, but no report was generated. In addition the inspection certificate is available here: