Specific Process Knowledge/Lithography/EBeamLithography/Cassettes: Difference between revisions
Appearance
| (4 intermediate revisions by the same user not shown) | |||
| Line 78: | Line 78: | ||
! Substrate size !! ID !! Slot ID !! Material !! Image !! Position indication !! Approximate offset [µm] !! PA to stage shift [µm] | ! Substrate size !! ID !! Slot ID !! Material !! Image !! Position indication !! Approximate offset [µm] !! PA to stage shift [µm] | ||
|- | |- | ||
| Chips || BM4P-509 || 3A, 3B, 3C, 3D || Ti || [[image:BM4P-509_cas.png| | | Chips || BM4P-509 || 3A, 3B, 3C, 3D || Ti || [[image:BM4P-509_cas.png|600px]] || [[image:BM4P-509 small.png|300px]] | ||
|| 3A: -810 µm | || 3A: -810 µm | ||
| Line 91: | Line 91: | ||
|- | |- | ||
| Chips || BM4P-510 || 3A, 3B, 3C, 3D || Ti || [[image:BM4P-510_cas.png| | | Chips || BM4P-510 || 3A, 3B, 3C, 3D || Ti || [[image:BM4P-510_cas.png|600px]] || [[image:BM4P-509 small.png|300px]] || | ||
|- | |- | ||
| 2" || BM6P-006 || 2A, 2B, 2C, 2D, 2E, 2F || Al || [[image:BM6P-006_cas.png| | | 2" || BM6P-006 || 2A, 2B, 2C, 2D, 2E, 2F || Al || [[image:BM6P-006_cas.png|600px]] || [[image:BM6P-502 small.png|300px]] || | ||
|- | |- | ||
| 2" || BM6P-502 || 2A, 2B, 2C, 2D, 2E, 2F || Ti || [[image:BM6P-502_cas.png| | | 2" || BM6P-502 || 2A, 2B, 2C, 2D, 2E, 2F || Ti || [[image:BM6P-502_cas.png|600px]] || [[image:BM6P-502 small.png|300px]] || | ||
|- | |- | ||
| 3" || BM4P-021 || 3A, 3B, 3C, 3D || Al || [[image:BM4P-021_cas.png| | | 3" || BM4P-021 || 3A, 3B, 3C, 3D || Al || [[image:BM4P-021_cas.png|600px]] || [[image:BM4P-509 small copy.png|300px]] || | ||
|- | |- | ||
| 3" || BM4P-025 || 3A, 3B, 3C, 3D || Al || [[image:BM4P-025_cas.png| | | 3" || BM4P-025 || 3A, 3B, 3C, 3D || Al || [[image:BM4P-025_cas.png|600px]] || [[image:BM4P-509 small copy.png|300px]] || | ||
|- | |- | ||
| 4" || BSPCL-520 || 4A, 4B, 4C || Ti || [[image:BSPCL-520_cas.png| | | 4" || BSPCL-520 || 4A, 4B, 4C || Ti || [[image:BSPCL-520_cas.png|600px]] || [[image:BSPCL-520 small.png|300px]] || Currently out of use | ||
|- | |- | ||
| 4" || BM2P-011 || 4D, 4E || Al || [[image:BM2P-011_cas.png| | | 4" || BM2P-011 || 4D, 4E || Al || [[image:BM2P-011_cas.png|600px]] || [[image:BM2P-011 small.png|300px]] || || 4D: (330,150) | ||
|- | |- | ||
| 6" || BW6-009 || 6A || Al || [[image:BW6-009.png| | | 6" || BW6-009 || 6A || Al || [[image:BW6-009.png|600px]] || [[image:BW6-009 small.png|300px]] || | ||
|- | |- | ||
| 6" || BW6-042 || 6A || Al || [[image:BW6-042_cas.png| | | 6" || BW6-042 || 6A || Al || [[image:BW6-042_cas.png|600px]] || [[image:BW6-009 small.png|300px]] || | ||
|- | |- | ||
| 8" || BSPCL-514 || 8A || Ti || [[image:BPSPCL-514_cas.png| | | 8" || BSPCL-514 || 8A || Ti || [[image:BPSPCL-514_cas.png|600px]] || [[image:BW6-009 small.png|300px]] || | ||
|- | |- | ||
| Mask || B6025-025 || || Ti || [[image:B6025-025.png| | | Mask || B6025-025 || || Ti || [[image:B6025-025.png|600px]] || (140.000, 120.000) || | ||
|} | |} | ||