Specific Process Knowledge/Characterization/XRD/XRD SmartLab: Difference between revisions
Appearance
| (2 intermediate revisions by 2 users not shown) | |||
| Line 16: | Line 16: | ||
[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=428 XRD SmartLab in LabManager] - requires login | [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=428 XRD SmartLab in LabManager] - requires login | ||
'''For XRD SmartLab Users at Nanolab:''' There's a bug in the software in the cleanroom, so the Parts Help doesn't show up with useful information about the optics used in Optical and Sample Alignment when you click the '?'. We copied the Parts Help from the newer XRD Rot Anode so you can the information: | |||
*On the Desktop of the Smartlab computer in the cleanroom | |||
*In the Cleanroom Drive under _Equipment/XRD/PartsHelp_fromXRDRotAnode_SLSII | |||
| Line 22: | Line 26: | ||
[http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XRD/Process_Info Process information] | [http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XRD/Process_Info Process information] | ||
The basic optical components and the automatic optical alignment steps are described here: | |||
[https://www.youtube.com/watch?v=AbM1TwG5HyU Optical alignment video on Rigaku's Youtube channel] | |||
The measurement settings and results of the pre-acceptance test are described in this document, also found on the Lab Manager: | The measurement settings and results of the pre-acceptance test are described in this document, also found on the Lab Manager: | ||
| Line 60: | Line 67: | ||
* Evaluation of [[Specific Process Knowledge/Characterization/XRD/XRD SmartLab/Instrumental broading in GiXRD|Instrumental broading in GiXRD]]. | * Evaluation of [[Specific Process Knowledge/Characterization/XRD/XRD SmartLab/Instrumental broading in GiXRD|Instrumental broading in GiXRD]]. | ||
==θ/2θ X-ray Diffraction== | |||
* Evaluation of [[Specific Process Knowledge/Characterization/XRD/XRD SmartLab/Instrumental broading in T2T|Instrumental broadening in symmetrical θ/2θ measurements]]. | |||
==Equipment performance and process related parameters== | ==Equipment performance and process related parameters== | ||