Jump to content

Specific Process Knowledge/Characterization/SEM Gemini 1/ma: Difference between revisions

Jmli (talk | contribs)
Created page with "= Safety= The SEM Gemini 1 is a state of the art High resolution SEM with latest technology on low acceleration voltage imaging. Compared to the Supra models in the cleanroom, the Gemini 1 features a lot of sophisticated features that require specific training in order to ensure: * Instrument safety: If not correctly operated, the instrument may suffer irreperable damage. * User value: The level of sophistication is very high so unless correctly instructed, chances are t..."
 
Jmli (talk | contribs)
No edit summary
 
(11 intermediate revisions by the same user not shown)
Line 1: Line 1:
= Safety=
Technical specification
The SEM Gemini 1 is a state of the art High resolution SEM with latest technology on low acceleration voltage imaging. Compared to the Supra models in the cleanroom, the Gemini 1 features a lot of sophisticated features that require specific training in order to ensure:
* Instrument safety: If not correctly operated, the instrument may suffer irreperable damage.
* User value: The level of sophistication is very high so unless correctly instructed, chances are that a certain mode may be incorrectly applied and the user will only waste time.


Below is a list of features or modes that require specific training in addition to the 'standard' training. All specific trainings will be added to the personal LabManager competence page. If a user is observed using the instrument without proper training, the competences will revoked.


==List of modes/features/detectors that require specific individual training ==
Sample requirements
Any sample allowed in the cleanroom can be imaged in Gemini 1.


# NanoVP mode: The use of the  
If you have any questions, please consult the persons responsible for the SEM.
# STEM detector
 
# BSED detector
Sample sizes:
# Loading 150 mm wafers
Up to 8" wafers (the ranges on the X and Y axes only provide full view of a 6" wafer)
# Loading
 
Vacuum modes:
 
The SEM is usually operated in high vacuum (HV) mode where the chamber pressure is somewhere in the 2*10-4 to 10-6 mbar range. For imaging of non-conducting samples the instrument can be operated at elevated chamber pressures in the variable pressure modes.
 
Lateral resolution:
The resolution is critically dependent on the type of sample and the SEM operator skills. In the best cases one may expect:
 
High Vacuum operation:
1.0 nm at 15 kV (Inlens detector and optimum working distance)
1.9 nm at 1 kV (Inlens detector and optimum working distance)
VP mode operation:
2.0 nm at 30 kV (VPSE detector and optimum working distance)
 
Acceleration voltage:
20 V - 30 kV
 
 
Detectors:
 
SE2: In chamber secondary electron detector
Inlens: Inlens secondary electron detector
ESB: Inlens backscatter electron detector
aBSD: Motorized and retractable 4 quadrant and annular backscattered electron detector
VPSE: Variable pressure secondary electron detector
STEM detector:
 
Stage:
The eucentric stage is centered at approximately (X=75,Y=75).
 
X range: 150 mm
Y range: 150 mm
Z range: 50 mm
Rotation: 360o
Tilt range: -? to ?
Airlock:
 
The SEM is equipped with an airlock that allows 150 mm wafers to be transferred to the SEM chamber without breaking the vacuum thus enabling samples to be exchanged in less than two minutes. The restriction on sample heights depends on what sample holder is used. If you have large and bulky samples, please consult with Nanolab staff before mounting/loading them.
 
 
Accuracy and reproducibility:
 
DTU Nanolab performs quality control of the SEM every third month. The control checks the resolution and lateral measurement accuracy. The quality control instruction and results can be found on the machine page in LabManager.
 
Additional equipment:
The Spicer Consulting SC24 EMI cancellation system consists of:
#
 
 
Instrument logon
 
Windows logon on the Operator station PC
Use the Windows logon 'sem' with password 'sem1'
 
SmartSEM logon
Use your own SmartSEM logon and password created at the training session
 
Sample mounting
 
The importance of correct sample mounting cannot be understated. This will ensure:
# Optimum image conditions in terms of surface grounding, sample access
# instrument safety
 
 
 
Sample transfer
 
Samples are generally loaded through the load lock so the users are not allowed to vent the SEM chamber. Certain sample holders, however, must be loaded through the SEM door - they are:
# The 200 mm wafer holder
# The STEM detector (requires specific training)
# The filter holder (not sure about the purpose)
Users who want to use the sample holders above must have specific rights and/or training.
 
 
The airlock
 
To enable the use of the airlock, press the ''Exchange'' button on the hardpanel