The ALD window for titanium dioxide (TiO<sub>2</sub>) ranges from 120 <sup>o</sup>C to 350 <sup>o</sup>C. | The ALD window for titanium dioxide (TiO<sub>2</sub>) ranges from 120 <sup>o</sup>C to 350 <sup>o</sup>C. | ||
| Line 51: | Line 49: | ||
</gallery> | </gallery> | ||
Evgeniy Shkondin, DTU Danchip, April-May 2014. | Evgeniy Shkondin, DTU Nanolab (former DTU Danchip), April-May 2014. | ||
| Line 75: | Line 73: | ||
<br clear="all" /> | <br clear="all" /> | ||
Evgeniy Shkondin, DTU Danchip, 2014. | Evgeniy Shkondin, DTU Nanolab (former DTU Danchip), 2014. | ||