Jump to content

Specific Process Knowledge/Thermal Process/Oxidation/Wet oxidation E1 furnace: Difference between revisions

From LabAdviser
Paphol (talk | contribs)
No edit summary
Mmat (talk | contribs)
mNo edit summary
 
(3 intermediate revisions by one other user not shown)
Line 1: Line 1:
=<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]]=
{{cc-nanolab}}


<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i>
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/Oxidation/Wet_oxidation_E1 click here]'''


An acceptance test was done after the installation in November 2021 by Tempress. For wet oxidation at 1050 C and 30 minutes, the thickness variation over a wafer was 1.3%(wafer in wafer), over the boat was 0.35%(wafer to wafer) and ran to ran was 0.64%.




[[File:Wet1050_Acceptance_test.PNG|1100x1100px|center|thumb|Acceptance test by Tempress from November 2021.]]
[[File:Wet1050_Acceptance_test.PNG|1100x1100px|center|thumb|Acceptance test by Tempress from November 2021.]]

Latest revision as of 19:19, 10 June 2025

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here


An acceptance test was done after the installation in November 2021 by Tempress. For wet oxidation at 1050 C and 30 minutes, the thickness variation over a wafer was 1.3%(wafer in wafer), over the boat was 0.35%(wafer to wafer) and ran to ran was 0.64%.


Acceptance test by Tempress from November 2021.