Created page with "=Oven 250C= 300x300px|thumb|Oven 250C for pretreatment in Cx-1 The oven is typically used for dehydration pretreatment, of Si and glass substrates, to promote the resist adhesion. We recommend placing the wafers in a metal carrier in the oven for at least for 4 hours, or overnight, and spin coat resist on them as soon as possible after removing them from the oven. The user manual, and contact information can be found..."
 
Jehem (talk | contribs)
 
Line 1: Line 1:
=Oven 250C=
=Oven 250C=
[[Image:Oven_250_degrees_for_pretreatment_cr3.jpg|300x300px|thumb|Oven 250C for pretreatment in Cx-1]]
[[Image:Oven_250_degrees_for_pretreatment_cr3.jpg|400px|thumb|Oven 250C for pretreatment in Cx-1]]
The oven is typically used for dehydration pretreatment, of Si and glass substrates, to promote the resist adhesion. We recommend placing the wafers in a metal carrier in the oven for at least for 4 hours, or overnight, and spin coat resist on them as soon as possible after removing them from the oven.
The oven is typically used for dehydration pretreatment, of Si and glass substrates, to promote the resist adhesion. We recommend placing the wafers in a metal carrier in the oven for at least for 4 hours, or overnight, and spin coat resist on them as soon as possible after removing them from the oven.