== Standard E-beam resists and process guidelines ==
== Standard E-beam resists and process guidelines ==


DTU Nanolab offers a limited number of standard EBL resist for our users. Our standard resist and process guidelines are summarized below. CSAR (AR-P 6200.09) is installed on Spin coater Gamma E-beam & UV for easy spin coating of 2", 4" and 6" substrates. Other substrate sizes or resist have to be used in the Labspin 2/3 coating systems. The standard resist bottles are stored in the chemical cupboard in E-4.
DTU Nanolab offers a limited number of standard EBL resist for our users. Our standard resist and process guidelines are summarized below. CSAR (AR-P 6200.09) is installed on Spin coater Gamma E-beam & UV for spin coating of 2", 4" and 6" substrates. Other substrate sizes or resist have to be used in the Labspin 2/3 coating systems. The standard resist bottles are stored in the chemical cupboard in E-4.




{|border="1" cellspacing="1" cellpadding="10" style="text-align:left;"  width="95%"
{|border="1" cellspacing="1" cellpadding="10" style="text-align:left;"
|-
|-


Line 41: Line 41:
*AR-600-71  
*AR-600-71  
*Remover 1165
*Remover 1165
|[[media:Process_Flow_CSAR.docx‎|Process Flow CSAR.docx‎]] <br> [[media:Process Flow CSAR ESPACER.docx|Process Flow CSAR with ESPACER]] <br> [[media:Process Flow CSAR with Al.docx|Process Flow CSAR with Al]] <br> [[media:Process_Flow_LOR5A_CSAR_Developer_TMAH_Manual.docx|Process Flow LOR5A with CSAR]] <br>  
|<br> [[media:Process Flow CSAR with Al.docx|Process Flow CSAR with Al]] <br> [[media:Process_Flow_LOR5A_CSAR_Developer_TMAH_Manual.docx|Process Flow LOR5A with CSAR]] <br>  


|-
|-
Line 84: Line 84:




{|border="1" cellspacing="1" cellpadding="3" style="text-align:left;" width="95%"
{|border="1" cellspacing="1" cellpadding="10" style="text-align:left;"  
|-
|-


Line 134: Line 134:
|-
|-
|-style="background:LightGrey; color:black"
|-style="background:LightGrey; color:black"
|'''[[Specific_Process_Knowledge/Lithography/mrEBL6000|mr EBL 6000.1]]'''
|'''mr EBL 6000.1'''
|Negative
|Negative
|[http://http://www.microresist.de/home_en.htm MicroResist]
|[http://http://www.microresist.de/home_en.htm MicroResist]
Line 159: Line 159:
|
|
|[[media:Process Flow HSQ.docx|process flow HSQ]]
|[[media:Process Flow HSQ.docx|process flow HSQ]]
[[/High resolution patterning with HSQ|High resolution patterning with HSQ]]


|-
|-