'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/FlipScribe click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/FlipScribe click here]''' | ||
=The Cleaver: | '''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.''' | ||
The Cleaver: FlipScribe is a scriber designed for cleaving/scribing wafers into smaller pieces without leaving any particles on the frontside of the sample. It works be scribing from the backside. The equipment is placed in the left drawer underneath | |||
=The Cleaver: FlipScribe= | |||
The Cleaver: FlipScribe is a scriber designed for cleaving/scribing wafers into smaller pieces without leaving any particles on the frontside of the sample. It works be scribing from the backside. The equipment is placed in the left drawer underneath fume hood 5: Special purposes. When operated the the Cleaver: Flip Scribe should always be placed inside Fume hood 5. | |||
[[File:flipscribe.JPG|400px]] | [[File:flipscribe.JPG|400px]] | ||