Specific Process Knowledge/Thin film deposition/Deposition of ZnO: Difference between revisions
No edit summary |
No edit summary |
||
| (One intermediate revision by one other user not shown) | |||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_ZnO click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_ZnO click here]''' | ||
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i> | |||
ZnO can be deposited by Sputtering process and atomic layer deposition (ALD). In the chart below you can compare the different deposition equipment. | =Zinc oxide (ZnO)= | ||
Zinc oxide (ZnO) is a wide‑bandgap (~3.3 eV) n‑type semiconductor that combines high visible transparency, decent carrier mobility, chemical stability, and notable piezoelectricity, while being abundant and non‑toxic. | |||
It is readily deposited by magnetron sputtering for uniform, large‑area films and by atomic layer deposition (ALD) for ultra‑conformal, low‑temperature coatings on complex, high‑aspect‑ratio structures. | |||
As a transparent thin film, ZnO serves as a window/contact in photovoltaics and LEDs and as a transparent electrode when adequately doped or hydrogenated to lower sheet resistance. | |||
In optics and photonics, ZnO functions as a high-index, low-loss dielectric for waveguides, tunable anti-reflective coatings, and Bragg mirrors; its stoichiometry and carrier density allow for control of the refractive index and absorption. | |||
Its piezoelectric and surface‑active nature underpins surface‑acoustic‑wave devices, microphones, nanogenerators, and highly responsive UV and gas sensors. | |||
Beyond these, polycrystalline ZnO varistors are standard for surge protection, and patterned or hybrid ZnO stacks enable transparent heaters, low-emissivity/IR-control, and EMI-shielding coatings, while offering good hardness and corrosion resistance. | |||
==Deposition of ZnO== | |||
ZnO can be deposited by the Sputtering process and atomic layer deposition (ALD). In the chart below, you can compare the different deposition equipment. | |||
*[[Specific Process Knowledge/Thin film deposition/ALD Picosun R200/ZnO deposition using ALD|ZnO deposition using ALD]] | *[[Specific Process Knowledge/Thin film deposition/ALD Picosun R200/ZnO deposition using ALD|ZnO deposition using ALD]] | ||
Latest revision as of 17:54, 28 July 2025
Feedback to this page: click here
Unless otherwise stated, this page is written by DTU Nanolab internal
Zinc oxide (ZnO)
Zinc oxide (ZnO) is a wide‑bandgap (~3.3 eV) n‑type semiconductor that combines high visible transparency, decent carrier mobility, chemical stability, and notable piezoelectricity, while being abundant and non‑toxic. It is readily deposited by magnetron sputtering for uniform, large‑area films and by atomic layer deposition (ALD) for ultra‑conformal, low‑temperature coatings on complex, high‑aspect‑ratio structures. As a transparent thin film, ZnO serves as a window/contact in photovoltaics and LEDs and as a transparent electrode when adequately doped or hydrogenated to lower sheet resistance. In optics and photonics, ZnO functions as a high-index, low-loss dielectric for waveguides, tunable anti-reflective coatings, and Bragg mirrors; its stoichiometry and carrier density allow for control of the refractive index and absorption. Its piezoelectric and surface‑active nature underpins surface‑acoustic‑wave devices, microphones, nanogenerators, and highly responsive UV and gas sensors. Beyond these, polycrystalline ZnO varistors are standard for surge protection, and patterned or hybrid ZnO stacks enable transparent heaters, low-emissivity/IR-control, and EMI-shielding coatings, while offering good hardness and corrosion resistance.
Deposition of ZnO
ZnO can be deposited by the Sputtering process and atomic layer deposition (ALD). In the chart below, you can compare the different deposition equipment.
| Sputtering deposition (Lesker) | Atomic layer deposition (ALD Picosun R200) | |
|---|---|---|
| General description | Sputter deposition of ZnO | Atomic layer deposition of ZnO |
| Pre-clean | RF Ar clean | |
| Layer thickness | 10Å to 5000Å* | 0 to 1000 Å |
| Deposition rate | Depending on process parameters. | Depending on temperature |
| Batch size |
|
|
| Allowed materials |
|
|
| Comment |
|
* For thicknesses above 200 nm permission is required.