Specific Process Knowledge/Thermal Process/Jipelec RTP: Difference between revisions
Appearance
mNo edit summary |
|||
| (2 intermediate revisions by 2 users not shown) | |||
| Line 1: | Line 1: | ||
{{cc-nanolab}} | |||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/Jipelec_RTP click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/Jipelec_RTP click here]''' | ||
'''<p style="color:red;"> The Jipelec RTP has been decomissioned in March 2023. It has been replaced with the Jipelec RTP2.</span>''' | |||
[[Category: Equipment |Thermal Jipelec]] | [[Category: Equipment |Thermal Jipelec]] | ||
| Line 6: | Line 12: | ||
==Jipelec - Rapid Thermal Processing== | ==Jipelec - Rapid Thermal Processing== | ||
[[Image:RTP_oven.jpg|300x300px|thumb|Jipelec RTP: Positioned in cleanroom A-4]] | [[Image:RTP_oven.jpg|300x300px|thumb|Jipelec RTP: Positioned in cleanroom A-4/ Photo: DTU Nanolab internal]] | ||
The Jipelec is a rapid thermal processing (RTP) oven. It is be used for fast and well-controlled annealing or alloying of samples. It is possible to use either a thermocouple or a pyrometer to control the temperature (of the sample carrier). | The Jipelec is a rapid thermal processing (RTP) oven. It is be used for fast and well-controlled annealing or alloying of samples. It is possible to use either a thermocouple or a pyrometer to control the temperature (of the sample carrier). | ||