Specific Process Knowledge/Cleanroom Chemicals: Difference between revisions
Appearance
mNo edit summary |
|||
| (7 intermediate revisions by 2 users not shown) | |||
| Line 1: | Line 1: | ||
=Chemicals in the Cleanroom (B346)= | |||
<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION.</span> | |||
This page lists the chemicals that are made available in the cleanroom by Nanolab, covered by the cleanroom access hourly rate. | This page lists the chemicals that are made available in the cleanroom by Nanolab, covered by the cleanroom access hourly rate. | ||
| Line 25: | Line 25: | ||
=Developers= | =Developers= | ||
*AR 600-546 (Amyl acetate). Stored in E-4 | *AR 600-546 (Amyl acetate). Stored in E-4 | ||
*AZ 351B (NaOH based with disodium tetraborate buffer). Stored in E-4. | *AZ 351B (NaOH based with disodium tetraborate buffer). Stored in E-4. | ||
*AZ 726 MIF (TMAH based with surfactants added for fast and homogeneous substrate wetting). Stored in E-4. | *AZ 726 MIF (TMAH based with surfactants added for fast and homogeneous substrate wetting). Stored in E-4. | ||
*mr-Dev 600 (PGMEA). Stored in Bx1. | *mr-Dev 600 (PGMEA). Stored in Bx1. Or E-4? | ||
*ZED-N50 (n-Amylacetate). Stored in E-4. | *ZED-N50 (n-Amylacetate). Stored in E-4. | ||
| Line 52: | Line 52: | ||
*Ethanol. Stored in C-1, D-3, E-4. | *Ethanol. Stored in C-1, D-3, E-4. | ||
*MIBK. Stored in E-4. | *MIBK. Stored in E-4. | ||
*PGMEA (available as mr-Dev 600). Stored in Bx1. | *PGMEA (available as mr-Dev 600). Stored in Bx1. Or E-4? | ||
*Remover 1165 (NMP). Stored in D-3, E-4. | *Remover 1165 (NMP). Stored in D-3, E-4. | ||
| Line 59: | Line 59: | ||
=Missing from list?= | =Missing from list?= | ||
* | *AP3000? | ||
*APS-100 (Ammonium persulfate based copper etch)? | |||
*AZ 400K (KOH based with Potassium borate buffer)? | |||
*Ethyl Acetate? | *Ethyl Acetate? | ||
*HSQ? | *HSQ? | ||
*Rinse T1100 (Mixture of Mesitylin, 1,2,4-Trimethylbenzene)? | |||
*UVN2300? | *UVN2300? | ||