=Convert data for loading in SmartLab Studio II= | =Convert data for loading in SmartLab Studio II= | ||
Data from the XRD Powder can be loading in the "Powder XRD" plugin in SmartLab Studio II. But the files have to be converted to a format read by SmartLab Studio II first. Two options are available for | Data from the XRD Powder can be loading in the "Powder XRD" plugin in SmartLab Studio II. But the files have to be converted to a format read by SmartLab Studio II first. Two options are available for conversion, Data Viewer provided by Malvern Panalytical or the opensource PowDLL developed at the University of Ioannina in Greece. You can see how to download these softwares in [https://labmanager.dtu.dk/view_binary.php?fileId=6287 this document] ''- requires login.'' | ||
==Converting to .xy with Data Viewer== | ==Converting to .xy with Data Viewer== | ||
Malvern Panalytical's Data Viewer can convert the xrdml files to xy files, which only consist of two columns with angles and intensities. No additional information is transferred in the xy format. The conversion is quite easy: | Malvern Panalytical's Data Viewer can convert the xrdml files to xy files, which only consist of two columns with angles and intensities. No additional information is transferred in the xy format. The conversion is quite easy: | ||
| Line 9: | Line 13: | ||
*Select X-Y table (*.xy) and deselect others. | *Select X-Y table (*.xy) and deselect others. | ||
*Click convert. | *Click convert. | ||
==Converting to .asc with PowDLL== | |||
PowDLL can convert to Rigaku's ascii format *.asc, which contains some information on the measurement setup. | |||
*Open PowDLL | |||
*Drag file or files from Windows Explore into PowDLL | |||
*Select Export format: "Rigaku ASC (*.asc)" | |||
*Click "Convert All Files" | |||
Latest revision as of 15:17, 31 March 2025
Feedback to this page: click here
Unless otherwise stated, this page is written by DTU Nanolab internal
Convert data for loading in SmartLab Studio II
Data from the XRD Powder can be loading in the "Powder XRD" plugin in SmartLab Studio II. But the files have to be converted to a format read by SmartLab Studio II first. Two options are available for conversion, Data Viewer provided by Malvern Panalytical or the opensource PowDLL developed at the University of Ioannina in Greece. You can see how to download these softwares in this document - requires login.
Converting to .xy with Data Viewer
Malvern Panalytical's Data Viewer can convert the xrdml files to xy files, which only consist of two columns with angles and intensities. No additional information is transferred in the xy format. The conversion is quite easy:
- Load xrdml file in Data Viewer.
- Select file -> convert.
- Select the output folder (I have problems save to my document folder).
- Select X-Y table (*.xy) and deselect others.
- Click convert.
Converting to .asc with PowDLL
PowDLL can convert to Rigaku's ascii format *.asc, which contains some information on the measurement setup.
- Open PowDLL
- Drag file or files from Windows Explore into PowDLL
- Select Export format: "Rigaku ASC (*.asc)"
- Click "Convert All Files"