== How to read the SPTS notation on process recipes ==
<!-- Page reviewed 9/8-2022 jmli -->
<!-- Page reviewed 28/6-2023 jmli -->
 
{{contentbydryetch}}
 
== How to read the notation on process recipes ==
<!-- revised 1/6-2015 by jmli -->
<!-- revised 1/6-2015 by jmli -->
To understand the SPTS short hand notation on process recipes look at two examples from the etch cycle of Step1 of the Process A shown in '''bold''' below:  
Look at two examples from the etch cycle of Step1 of the Process A shown in '''bold''' below:  
# The Platen power has the setting ''120 >> 140 (1.5s) 45 '' - it is to be interpreted as:
# The Platen power has the setting ''120 >> 140 (1.5s) 45 '' - it is to be interpreted as:
## In the first 1.5 seconds of the every cycle the platen power has a value that is ramped (indicated by >>) from 120 W initially to 150 W in the end
## In the first 1.5 seconds of the every cycle the platen power has a value that is ramped (indicated by >>) from 120 W initially to 150 W in the end
Line 59: Line 65:
|-
|-
| Common  
| Common  
| colspan="4" | Temperature 20 degs, HBC 10 torr, Short funnel, with baffle & 5mm spacers
| colspan="4" | Temperature 20 degs, HBC 10 torr
|}
|}