Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange/ProcessD/PrD-4: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
No edit summary
Jmli (talk | contribs)
No edit summary
 
(2 intermediate revisions by the same user not shown)
Line 1: Line 1:
<!-- Ok, jmli 20170627 -->
<!-- Ok, jmli 20170627 -->
<!-- Page reviewed 9/8-2022 jmli -->
<!--Page reviewed by jmli 28/4-2023  -->
{{Author-jmli1}}
<!--Checked for updates on 4/9-2025 - ok/jmli -->


{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;"
{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;"

Latest revision as of 10:32, 4 September 2025

Unless otherwise stated, all content on this page was created by Jonas Michael-Lindhard, DTU Nanolab


Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
8/1-2015 4" Wafer with travkaXX mask AZ standard Si / XX % Pegasus/jmli s004781 nanolab/jml/showerhead/prD/PrD-4, 150 cyc or 8:00 mins S004782 New showerhead