Specific Process Knowledge/Characterization/Element analysis: Difference between revisions
Appearance
| (2 intermediate revisions by one other user not shown) | |||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:characterization@ | '''Feedback to this page''': '''[mailto:characterization@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/Element_analysis&action=edit click here]''' | ||
<!--Checked for updates on 24/8-2021. ok/ jmli--> | |||
| Line 7: | Line 7: | ||
The following techniques for elemental analysis are available at Nanolab. | The following techniques for elemental analysis are available at Nanolab. | ||
* EDX | * EDX | ||
* SIMS (no longer available at Nanolab, SIMS service can be provided by | * SIMS (no longer available at DTU Nanolab, SIMS service can be provided by [http://www.eag.com/ EAG Laboratories]) | ||
* XPS (ESCA) | * XPS (ESCA) | ||
In the table below the three techniques are compared | In the table below the three techniques are compared | ||
| Line 13: | Line 13: | ||
== Comparison of EDX, SIMS and XPS == | == Comparison of EDX, SIMS and XPS == | ||
{| border="2" cellspacing="0" cellpadding="2" align=" | {| border="2" cellspacing="0" cellpadding="2" align="left" | ||
!width="100" style="background:silver; color:black" | | !width="100" style="background:silver; color:black" | | ||
!width="250" style="background:silver; color:black" | SEM with [[Specific Process Knowledge/Characterization/EDX|EDX]] | !width="250" style="background:silver; color:black" | SEM with [[Specific Process Knowledge/Characterization/EDX|EDX]] | ||