'''Feedback to this page''': '''[mailto:thinfilm@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/Resist_Pyrolysis_Furnace click here]''' | '''Feedback to this page''': '''[mailto:thinfilm@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/Resist_Pyrolysis_Furnace click here]''' | ||
''This page is written by DTU Nanolab internal'' | |||
===<span style="color:Red">EXPIRED! | ===<span style="color:Red">EXPIRED! | ||
This page contains information about an old resist pyrolysis furnace that was removed from the cleanroom August 2019. Use the new Resist Pyrolysis furnace (former Multipurpose Anneal furnace) instead.</span>=== | |||
| Line 9: | Line 11: | ||
[[Category: Thermal process|Resist Pyrolysis]] | [[Category: Thermal process|Resist Pyrolysis]] | ||
[[Category: Furnaces|Resist Pyrolysis]] | [[Category: Furnaces|Resist Pyrolysis]] | ||
== Resist Pyrolysis Furnace == | == Resist Pyrolysis Furnace == | ||