Specific Process Knowledge/Back-end processing/Polisher CMP: Difference between revisions
No edit summary |
|||
(One intermediate revision by the same user not shown) | |||
Line 1: | Line 1: | ||
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.''' | |||
'''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.''' | |||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/Polisher_CMP click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/Polisher_CMP click here]''' | ||
Line 8: | Line 13: | ||
[[image:Cmp_picture.jpg|400px|right|thumb|The Logitech PM5 Polisher/Lapper in cleanroom A-5]] | [[image:Cmp_picture.jpg|400px|right|thumb|The Logitech PM5 Polisher/Lapper in cleanroom A-5]] | ||
The Logitech Orbis Polisher (CMP) is for polishing wafers (removing material in the nm range) it is not for thinning down wafers or other substrates. | The Logitech Orbis Polisher (CMP) is for polishing wafers (removing material in the nm range) it is not for thinning down wafers or other substrates. After CMP it is recommended to use the '''[http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Wafer_cleaning/Post_CMP_Cleaner Post CMP Cleaner]''' to clean the sample for slurry residues left by the CMP. | ||
Latest revision as of 16:21, 6 February 2023
Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.
All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.
Feedback to this page: click here
Polisher (CMP)

The Logitech Orbis Polisher (CMP) is for polishing wafers (removing material in the nm range) it is not for thinning down wafers or other substrates. After CMP it is recommended to use the Post CMP Cleaner to clean the sample for slurry residues left by the CMP.
The user manual, user APV, technical information and contact information can be found in LabManager:
The Logitech Orbis (CMP) in LabManager
Equipment | Polisher/Lapper | |
---|---|---|
Purpose |
Polishing of |
|
Performance | 20x20mm substrate |
|
100mm substrate |
| |
Process parameter range | Polishing liquid |
|
Polishing cloths |
| |
Rotation |
| |
Arm sweep |
| |
Substrates | Sample size |
|
Allowed materials |
|