Specific Process Knowledge/Characterization/XPS/Processing: Difference between revisions
Appearance
No edit summary |
|||
| (68 intermediate revisions by 3 users not shown) | |||
| Line 2: | Line 2: | ||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XPS/Processing click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XPS/Processing click here]''' | ||
<!-- Page reviewed 8/5-2023 jmli --> | |||
<!--Checked for updates on 9/5-2023 - ok/jmli --> | |||
<!--Checked for updates on 5/2-2026 - ok/jmli --> | |||
{{Contentbydryetch}} | |||
= | = XPS Data processing with Avantage = | ||
== How to analyze data== | |||
In this section, all steps (import data, add peaks and backgrounds etc.) of the analysis are described. | |||
== | === XPS Simplified === | ||
The web page [https://xpssimplified.com/index.php XPS Simplified] is a ThermoScientific page where you can find a lot of information about the techniques, the hardware, data analysis etc. | |||
=== | === XPS Knowledge View === | ||
A knowledge database providing specific information on every element is included in the software. It provides very useful information about the XPS characteristics of every detectable element and it may even be a very good idea to consult it before the data is acquired. Click [[Specific Process Knowledge/Characterization/XPS/Processing/XPSknowledgeview|HERE]] to get information on how to access XPS Knowledge View in Avantage. | A knowledge database providing specific information on every element is included in the software. It provides very useful information about the XPS characteristics of every detectable element and it may even be a very good idea to consult it before the data is acquired. Click [[Specific Process Knowledge/Characterization/XPS/Processing/XPSknowledgeview|'''HERE''']] to get information on how to access XPS Knowledge View in Avantage. | ||
=== | === Basic instructions === | ||
Click [[Specific Process Knowledge/Characterization/XPS/Processing/Basics|'''HERE''']] to have a complete walk-through of an example. This includes | Click [[Specific Process Knowledge/Characterization/XPS/Processing/Basics|'''HERE''']] to have a complete walk-through of an example. This includes | ||
| Line 34: | Line 31: | ||
** Quantify | ** Quantify | ||
* Analyze depth profiles | * Analyze depth profiles | ||
=== Guidelines on data processing === | |||
Click [[Specific Process Knowledge/Characterization/XPS/Processing/Guidelines|'''HERE''']] to see some general guidelines on data processing in Avantage. | |||
== Introduction to data analysis with Avantage by Thermofisher == | |||
In the Youtube video below, the application specialist from Thermorfisher Paul Mack walks you through Avantage...somewhat slowly.. | |||
[https://www.youtube.com/watch?v=gVzYThRKjYQ '''Click here '''] | |||
== Examples of data analysis == | == Examples of data analysis == | ||
*[[Specific Process Knowledge/Characterization/XPS/Processing/ | *[[Specific Process Knowledge/Characterization/XPS/Processing/ALDSandwich1|Depth profile of ALD layers: Silicon wafer with 15 nm Al<sub>2</sub>O<sub>3</sub>, 15 nm of TiO<sub>2</sub> and 16 nm of HfO<sub>2</sub> ]] | ||
*[[ | *[[Specific_Process_Knowledge/Characterization/XPS/XPS_Depth_profiling|Depth profile of a silicon wafer with nitride, polysilicon and oxide layer]] | ||
== Periodic table with binding energies of all elements== | == Periodic table with binding energies of all elements== | ||
*[[Specific Process Knowledge/Characterization/XPS/Processing/PeriodicTable]] | *[[Specific Process Knowledge/Characterization/XPS/Processing/PeriodicTable]] | ||
= XPS data analysis with CasaXPS = | |||
CasaXPS has its own [https://www.youtube.com/channel/UCUqLBeW-UAjXC55HbRYOabQ Youtube channel] with more than 250 videos so it would be a complete waste of time to make any instructions here. Instead, this is where you as a CasaXPS user could contribute to this database: In case you found any Youtube video that was particularly good, please notify us and we will post a link. | |||
In order to use CasaXPS, you will need to export the data from Avantage and convert it into the Vamas format. Click [[Specific Process Knowledge/Characterization/XPS/Export2CasaXPS | ''this link'']] to find more information. | |||