Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/ProcessA/ProcessLog: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
No edit summary
Jmli (talk | contribs)
Replaced content with "'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/ProcessA/ProcessLog click here]''' <!--Checked for updates on 30/7-2018 - ok/jmli --> <!--Checked for updates on 5/10-2020 - ok/jmli --> <!--Checked for updates on 21/10-2025. ok/ jmli-->"
Tag: Replaced
 
(One intermediate revision by the same user not shown)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/ProcessA/ProcessLog click here]'''
<!--Checked for updates on 30/7-2018 - ok/jmli -->
<!--Checked for updates on 30/7-2018 - ok/jmli -->
 
<!--Checked for updates on 5/10-2020 - ok/jmli -->
{| {{table}}
<!--Checked for updates on 21/10-2025. ok/ jmli-->
| align="center" style="background:#f0f0f0;"|'''End date'''
| align="center" style="background:#f0f0f0;"|'''User'''
| align="center" style="background:#f0f0f0;"|'''line'''
| align="center" style="background:#f0f0f0;"|'''noProcessingDone [text]'''
| align="center" style="background:#f0f0f0;"|'''Etched material [list+]'''
| align="center" style="background:#f0f0f0;"|'''Mask material [list+]'''
| align="center" style="background:#f0f0f0;"|'''Recipe [text]'''
| align="center" style="background:#f0f0f0;"|'''Wafer ID [text]'''
| align="center" style="background:#f0f0f0;"|'''Process time [m]'''
| align="center" style="background:#f0f0f0;"|'''Process time [s]'''
| align="center" style="background:#f0f0f0;"|'''Process time [hh:mm:ss calc]'''
| align="center" style="background:#f0f0f0;"|'''Chiller temperature [°C]'''
| align="center" style="background:#f0f0f0;"|'''Comments [text]'''
|-
| 02-05-2016 14:50||jmli||1||||None||None||HiLi10mins||none||10||0||00:10:00||0||
|-
| 02-05-2016 14:50||jmli||2||||4" Si||Az 4562||PrA-0||C03991.01||14||40||00:14:40||20||Travka20 wafer, 80cyc step2;
|-
| 02-05-2016 14:50||jmli||3||||None||None||3min TDESC clean||none||3||0||00:03:00||0||
|-
| 02-05-2016 14:50||jmli||4||||4" Si||Az 4562||PrA-1||C03991.02||14||0||00:14:00||20||Travka20 wafer, 80cyc step2;
|-
| 02-05-2016 14:50||jmli||5||||None||None||HiLi10mins||none||10||0||00:10:00||0||
|-
| 02-05-2016 14:50||jmli||6||||4" Si||Az 4562||PrA-2||C03991.03||14||40||00:14:40||20||Travka20 wafer, 80cyc step2;
|-
| 02-05-2016 14:50||jmli||7||||None||None||3min TDESC clean||none||3||0||00:03:00||0||
|-
| 02-05-2016 14:50||jmli||8||||4" Si||Az 4562||PrA-0||C03991.04||14||40||00:14:40||20||Travka20 wafer, 80cyc step2;
|-
| 02-05-2016 14:50||jmli||9||||None||None||3min TDESC clean||none||3||0||00:03:00||0||
|-
| 02-05-2016 14:50||jmli||10||||4" Si||Az 4562||PrA-1||C03991.05||14||0||00:14:00||20||Travka20 wafer, 80cyc step2;
|-
| 02-05-2016 14:50||jmli||11||||None||None||3min TDESC clean||none||3||0||00:03:00||0||
|-
| 02-05-2016 14:50||jmli||12||||4" Si||Az 4562||PrA-2||C03991.06||14||40||00:14:40||20||Travka20 wafer, 80cyc step2;
|-
| 02-05-2016 14:50||jmli||13||||None||None||HiLi10mins||none||10||0||00:10:00||0||
|-
| 03-06-2016 14:47||jmli||1||||None||None||3min TDESC clean||none||3||0||00:03:00||20||
|-
| 03-06-2016 14:47||jmli||2||||Si||Az Mir 701||PrA-0||C04047.01||14||40||00:14:40||20||travka20 wafer
|-
| 03-06-2016 14:47||jmli||3||||None||None||3min TDESC clean||none||3||0||00:03:00||20||
|-
| 03-06-2016 14:47||jmli||4||||Si||Az Mir 701||PrA-1||C04047.02||14||40||00:14:40||20||travka20 wafer
|-
| 03-06-2016 14:47||jmli||5||||None||None||3min TDESC clean||none||3||0||00:03:00||20||
|-
| 03-06-2016 14:47||jmli||6||||Si||Az Mir 701||PrA-2||C04047.03||14||40||00:14:40||20||travka20 wafer
|-
| 03-06-2016 14:47||jmli||7||||None||None||3min TDESC clean||none||3||0||00:03:00||20||
|-
| 03-06-2016 14:47||jmli||8||||Si||Az Mir 701||PrA-0||C04047.04||14||40||00:14:40||20||travka20 wafer
|-
| 03-06-2016 14:47||jmli||9||||None||None||3min TDESC clean||none||3||0||00:03:00||20||
|-
| 03-06-2016 14:47||jmli||10||||Si||Az Mir 701||PrA-1||C04047.05||14||40||00:14:40||20||travka20 wafer
|-
| 03-06-2016 14:47||jmli||11||||None||None||3min TDESC clean||none||3||0||00:03:00||20||
|-
| 03-06-2016 14:47||jmli||12||||Si||Az Mir 701||PrA-2||C04047.06||14||40||00:14:40||20||travka20 wafer
|-
| 03-06-2016 14:47||jmli||13||||None||None||3min TDESC clean||none||3||0||00:03:00||20||
|-
|
|}