Jump to content

Specific Process Knowledge/Etch/Wet Gold Etch: Difference between revisions

Choi (talk | contribs)
Taran (talk | contribs)
No edit summary
 
(5 intermediate revisions by 3 users not shown)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:wetchemistry@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Wet_Gold_Etch click here]'''
'''Feedback to this page''': '''[mailto:wetchemistry@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Wet_Gold_Etch click here]'''


[[Category: Equipment|Etch Wet Gold]]
'''Unless anything else is stated, everything on this page text and pictures are made by DTU Nanolab.'''
[[Category: Etch (Wet) bath|Gold]]
 
'''All links to Kemibrug (SDS) and Labmanager Including APV requires login.'''
 
'''All measurements on this page has been made by Nanolab staff.'''
 
[[Category:Equipment|Etch Wet Gold]]
[[Category:Etch (Wet) bath|Gold]]


Ething of Gold can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done with [[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE]] by sputtering with Ar ions.  
Ething of Gold can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done with [[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE]] by sputtering with Ar ions.  
Line 13: Line 19:
We have two different solutions:
We have two different solutions:


# Iodine etch: KI:I<sub>2</sub>:H<sub>2</sub>O - 100g:25g:500ml - standard at Danchip. Can be used with AZ resist as mask.
# Iodine etch: KI:I<sub>2</sub>:H<sub>2</sub>O - 100g:25g:500ml - standard at DTU Nanolab. Can be used with AZ resist as mask.
# Aqua Regia (Kongevand): HNO<sub>3</sub>:HCl - 1:3 - A very strong acid which will etch most metals and is therefore used when you wish to remove all the gold from your wafer. '''You must be very careful when working with Aqua Regia (Kongevand). It can generate nitrogen oxide gases which are very toxic!!'''
# Aqua Regia (Kongevand): HNO<sub>3</sub>:HCl - 1:3 - A very strong acid which will etch most metals and is therefore used when you wish to remove all the gold from your wafer. '''You must be very careful when working with Aqua Regia (Kongevand). It can generate nitrogen oxide gases which are very toxic!'''