Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange/ProcessD/PrD-4: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| (4 intermediate revisions by the same user not shown) | |||
| Line 1: | Line 1: | ||
<-- Ok, jmli 20170627 /--> | <!-- Ok, jmli 20170627 --> | ||
<!-- Page reviewed 9/8-2022 jmli --> | |||
<!--Page reviewed by jmli 28/4-2023 --> | |||
{{Author-jmli1}} | |||
<!--Checked for updates on 4/9-2025 - ok/jmli --> | |||
{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" | {| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" | ||
| Line 24: | Line 30: | ||
| Pegasus/jmli | | Pegasus/jmli | ||
| s004781 | | s004781 | ||
| | | nanolab/jml/showerhead/prD/PrD-4, 150 cyc or 8:00 mins | ||
| S004782 | | S004782 | ||
! New showerhead | ! New showerhead | ||