Specific Process Knowledge/Etch/DRIE-Pegasus/Isotropic/Isoslow7: Difference between revisions
Appearance
Created page with "{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" |+ '''Process runs''' |- ! rowspan="2" width="40"| Date ! colspan="4" width="120"| Substrate Informati..." |
No edit summary |
||
| (2 intermediate revisions by the same user not shown) | |||
| Line 1: | Line 1: | ||
'''Feedback to this page''': | |||
'''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/Isotropic/Isolslow7 click here]''' | |||
<!--Checked for updates on 30/7-2018 - ok/jmli --> | |||
<!--Checked for updates on 5/10-2020 - ok/jmli --> | |||
<!--Checked for updates on 4/4-2025 - ok/jmli --> | |||
{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" | {| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" | ||
|+ '''Process runs''' | |+ '''Process runs''' | ||
Latest revision as of 08:27, 4 April 2025
Feedback to this page: click here
| Date | Substrate Information | Process Information | SEM Images | ||||||
|---|---|---|---|---|---|---|---|---|---|
| Wafer info | Mask | Material/ Exposed area | Tool / Operator | Conditioning | Recipe | Wafer ID | Comments | ||
| 28/2-2014 | 4" | travka50 wafer 1.5 µm AZ | Si / 50 % | Pegasus/jmli | 1 minute TDESC clean + MU runs | jml/isotropic/isoslow7 1:00 minutes | S003900 | Bottom fine!! | |