Jump to content

Specific Process Knowledge/Characterization/SEM Supra 2: Difference between revisions

Pevo (talk | contribs)
No edit summary
Pevo (talk | contribs)
 
(24 intermediate revisions by 3 users not shown)
Line 1: Line 1:
=<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]]=


'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/SEM_Supra_2  click here]'''


'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/SEM_Supra_2 click here]'''
''This page is written by DTU Nanolab internal''


'''The user manuals, quality control procedures and results, user APVs, technical information and contact information can be found in LabManager:'''<br>
[[image:SEM_Supra_2.jpg|500x500px|right|thumb|The SEM Supra 2 is located in cleanroom C-1. {{photo1}} ]]


SEM's at DTU Danchip:
=SEM Supra 2=
* [http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=37| The SEM Leo page in LabManager],
* [http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=275| The SEM Supra 1 page in LabManager],
* [http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=327| The SEM Supra 2 page in LabManager],
* [http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=361| The SEM Supra 3 page in LabManager],


The SEM Supra 2 is a scanning electron microscope. It produces enlarged images of a variety of specimens, achieving magnifications of over 500.000x providing ultra high resolution imaging. This important and widely used analytical tool provides exceptional resolution and depth of field and requires minimal specimen preparation.


==Equipment performance and process related parameters==
The SEM is a VP (variable pressure) instrument - Indicating that it is capable of operating at variable pressure. By increasing the pressure in the chamber it is possible to image isolating samples. The higher density of gas molecules will eliminate the charges at the cost of slightly reduced resolution. Also, the SE2 and InLens detectors will no longer work, and a dedicated VPSE detector have to be used instead.
 
This SEM has large chamber volume compared to the other SEM's in the cleanroom at DTU Nanolab. An 8" wafer can be loaded in the chamber, however the X and Y ranges only provide full view of a 6" wafer.
 
All samples must be introduced into the chamber using an airlock. The airlock greatly reduces sample exchange times, and it accepts up to 8" wafer holders.
 
The SEM is equipped with an Oxford Instruments Aztec Advanced Ultim 65 mm2 SDD EDX detector and Aztec software. EDX (Energy dispersive X-ray) detection is used for element composition analysis in a small area. A specific training is needed for users that want to use the EDX detector. 
 
The SEM Supra 2 in located in the cleanroom. It was installed in December 2013.
 
 
'''The user manual, control instruction, the user APV and contact information can be found in LabManager:'''
 
[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=327 SEM Supra 2 info page in LabManager]
 
 
== Performance information ==
 
*[[Specific Process Knowledge/Characterization/SEM: Scanning Electron Microscopy|SEM comparison page]]
 
*[[Specific Process Knowledge/Characterization/EDX|Energy Dispersive X-ray analysis (EDX)]]
 
 
==Equipment performances==


{| border="2" cellspacing="0" cellpadding="2"  
{| border="2" cellspacing="0" cellpadding="2"  


!colspan="2" border="none" style="background:silver; color:black;" align="center"|Equipment  
!colspan="2" border="none" style="background:silver; color:black;" align="center"|Equipment  
|style="background:WhiteSmoke; color:black"|<b>SEM Supra 1 (Supra 40VP SEM)</b>
|style="background:WhiteSmoke; color:black"|<b>SEM Supra 2 </b>
|-
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="1"|Purpose
!style="background:silver; color:black" align="center" valign="center" rowspan="1"|Purpose
|style="background:LightGrey; color:black"|Imaging and measurement of
|style="background:LightGrey; color:black"|Imaging and measurement of
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Any sample except bulk insulators such as polymers, glass or quartz wafers
* Conducting samples
* Semi-conducting samples
* Thin (~ 5 µm <) layers of non-conducting materials such as polymers
* Thick polymers, glass or quartz samples
|-
|-
!style="background:silver; color:black;" align="center" width="60"|Location  
!style="background:silver; color:black;" align="center" width="60"|Location  
|style="background:LightGrey; color:black"|
|style="background:LightGrey; color:black"|
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Basement of DTU Danchip
*Cleanroom of DTU Nanolab
|-
|-
!style="background:silver; color:black;" align="center" width="60"|Performance
!style="background:silver; color:black;" align="center" width="60"|Performance
Line 34: Line 57:
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*1-2 nm (limited by vibrations)
*1-2 nm (limited by vibrations)
The resolution is strongly dependent on the type of sample and the skills of the operator.
The resolution is strongly dependent on the SEM settings, the sample type and the skills of the operator
|-
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="5"|Instrument specifics
!style="background:silver; color:black" align="center" valign="center" rowspan="5"|Instrument specifics
|style="background:LightGrey; color:black"|Detectors
|style="background:LightGrey; color:black"|Detectors
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Secondary electron (Se2)
*Secondary electron (SE2)
*Inlens secondary electron (Inlens)
*Inlens secondary electron (Inlens)
*4 Quadrant Backscatter electron (QBSD)
*Variable pressure secondary electron (VPSE)
*Variable pressure secondary electron (VPSE)
|-
|-
|style="background:LightGrey; color:black"|Stage
|style="background:LightGrey; color:black"|Stage
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*X, Y: 130 &times; 130 mm
*X, Y: 150 mm &times; 150 mm
*T: -4 to 70<sup>o</sup>
*T: -10 to 70<sup>o</sup>
*R: 360<sup>o</sup>
*R: 360<sup>o</sup>
*Z: 50 mm
*Z: 50 mm
Line 57: Line 79:
|style="background:LightGrey; color:black"|Operating pressures
|style="background:LightGrey; color:black"|Operating pressures
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Fixed at High vacuum (2 &times; 10<sup>-4</sup>mbar - 10<sup>-6</sup>mbar)
*Fixed at High vacuum (2 &times; 10<sup>-4</sup >mbar - 10<sup>-6</sup> mbar)
*Variable at Low vacuum (0.1 mbar - 2 mbar)
*Variable at Low vacuum (0.1 mbar - 2 mbar)
|-
|-
|style="background:LightGrey; color:black"|Options
|style="background:LightGrey; color:black"|Options
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*All software options available
*Antivibration platform
*Fjeld M-200 airlock taking up to 8" wafers
*Oxford Instruments Aztec Advanced Ultim 65 mm<sup>2</sup> SDD EDX detector and Aztec software package
|-
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates
|style="background:LightGrey; color:black"|Batch size
|style="background:LightGrey; color:black"|Batch size
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Up to 6" wafer with full view  
*Up to 8" wafer with 6" view
|-
|-
| style="background:LightGrey; color:black"|Allowed materials
| style="background:LightGrey; color:black"|Allowed materials
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Any standard cleanroom material and samples from the Laser Micromachining tool and the Polymer Injection Molding tool
*Any standard cleanroom material
|-  
|-  
|}
==Quality control of length measurements ==
{| border="1" cellspacing="2" cellpadding="2" colspan="3"
|bgcolor="#98FB98" |'''Quality Control (QC) for SEM Supra 2'''
|-
|
*[http://labmanager.dtu.dk/d4Show.php?id=3531&mach=327 QC procedure for SEM Supra 2]<br>
*[https://labmanager.dtu.dk/view_binary.php?type=data&mach=327 Newest QC data for SEM Supra 2]<br>
'''QC limits:'''
{| {{table}}
| align="center" valign="top"|
{| border="2" cellspacing="1" cellpadding="2" align="center" style="width:500px"
! Detector
! Settings
! Magnification
! Measured dimensions
! Calibration limit
! Action limit
|-
|SE2
| EHT 10 kV, WD 10 mm
| 2.500 k
| 70x70 μm
| ± 2 %
| ± 3 %
|-
|SE2
| EHT 10 kV, WD 10 mm
| 17.000 k
| 10x10 μm
| ± 2 %
| ± 3 %
|-
|-
|SE2
| EHT 10 kV, WD 10 mm
| 75.000 k
| 2x2 μm
| ± 2 %
| ± 3 %
|-
|SE2
| EHT 5 kV, WD 5 mm
| 17.000 k
| 10x10 μm
| ± 2 %
| ± 3 %
|-
| VPSE
| EHT 10 kV, WD 10 mm, 17 Pa
| 17.000 k
| 10x10 μm
| ± 2 %
| ± 3 %
|-
| InLens
| EHT 5 kV, WD 5 mm
| 200.000 k
| 1x1 μm
| ± 2 %
| ± 3 %
|-
| InLens
| EHT 10 kV, WD 3 mm
| 1.000.000 k
| (imaging only)
| NA
| NA
|-
|}
|-
|}
|}
|}