| '''Feedback to this page''': '''[mailto:pvd@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_TiW&action=edit click here]''' | | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_TiW click here]''' |
| | |
| | |
| Deposition of TiW alloy can be done in the Wordentec.
| |
| | |
| | |
| '''Observe:''' ''right now we don´t have a TiW target for Wordentec, please contact thinfilm@danchip.dtu.dk if you are interested in depositing TiW.''
| |
|
| |
|
| | <i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i> |
|
| |
|
| ==Sputtering of TiW== | | ==Sputtering of TiW== |
|
| |
|
| * [[/Sputtering of TiW in Wordentec|Sputtering of TiW in Wordentec]]
| | Deposition of TiW alloy was done in the past in the [[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]]. This tool is now decommissioned, and if necessary processes may be developed for depositing TiW in the Lesker sputter setups (contact responsible staff for this). |
| | |
| | |
| | |
| {| border="1" cellspacing="0" cellpadding="4"
| |
|
| |
| |-style="background:silver; color:black"
| |
| |
| |
| ! Sputter deposition (Wordentec)
| |
| |-style="background:WhiteSmoke; color:black"
| |
| ! General description
| |
| | Sputter deposition of TiW
| |
| |-
| |
| |-style="background:LightGrey; color:black"
| |
| ! Pre-clean
| |
| |RF Ar clean
| |
| |-
| |
| | |
| |-style="background:WhiteSmoke; color:black"
| |
| ! Layer thickness
| |
| |.
| |
| |-
| |
| | |
| |-style="background:LightGrey; color:black"
| |
| | |
| ! Deposition rate
| |
| |Depending on process parameters, see [[/Sputtering of TiW in Wordentec|here.]]
| |
| |-
| |
| | |
| |-style="background:WhiteSmoke; color:black"
| |
| ! Batch size
| |
| |
| |
| *24x2" wafers or
| |
| *6x4" wafers or
| |
| *6x6" wafers
| |
| |-
| |
| | |
| |-style="background:LightGrey; color:black"
| |
| ! Allowed substrates
| |
| | |
| |
| |
| * Silicon wafers
| |
| * Quartz wafers
| |
| * Pyrex wafers
| |
| | |
| |-style="background:WhiteSmoke; color:black"
| |
| !Allowed materials
| |
| |
| |
| * Silicon oxide
| |
| * Silicon (oxy)nitride
| |
| * Photoresist
| |
| * PMMA
| |
| * Mylar
| |
| * SU-8
| |
| * Metals
| |
| |-
| |
| | |
| | |
| |-style="background:LightGrey; color:black"
| |
| ! Comments
| |
| | TiW alloy: 10%/90% by weight
| |
| |}
| |
| | |
| | |
| '''Deposited rates'''
| |
| | |
| This is done by a sputtering process. Process parameters (argon pressure and effect) can be varied, the surface roughness and the deposition rate (see [[/Sputtering of TiW in Wordentec|here]]) and may change with these settings. | |
| | |
| | |
| '''Deposited film characteristics'''
| |
|
| |
|
| AFM pictures show how the surface roughness is dependent of the process parameters, this can be seen here.
| | *[[/Sputtering of TiW in Wordentec|Sputtering of TiW in Wordentec]] |
| | *[[Specific Process Knowledge/Thin film deposition/Deposition of TiW/Sputtering of TiW in Wordentec/Grain size and uniformity of TiW layers|Results of a study on the grain size and uniformity of TiW sputtered in the Wordentec]] |