= PolyFabLab =
= Polymer Processing =
<span style="background:#FF2800">'''THIS PAGE IS UNDER CONSTRUCTION'''</span>


==UV lithography==
Polymer processing involves transforming polymer resins into finished products with desired shapes, dimensions and performance characteristics. It combines the principles of polymer science, heat transfer, fluid mechanics, and manufacturing technology to produce a wide range of components for various applications. The processing conditions, such as temperature, pressure, and cooling rate, significantly influence the final properties of the polymer product.
*[[Specific_Process_Knowledge/Lithography/UVExposure/aligner_MA6-1|Mask Aligner: MA6-1]]
 
*[[Specific_Process_Knowledge/Lithography/UVExposure/aligner_MLA4|Maskless Aligner: μMLA-04]]
There is a wide range of methods available to structure and modify polymers, though commonly done outside of a cleanroom, whereas some can be done inside a cleanroom.
*[[Specific_Process_Knowledge/Lithography/Coaters/labspin04]]
*[[Specific Process Knowledge/Lithography/NanoImprintLithography|Nano Imprint Lithography]]


==Additive Methods==
Many polymer processing methods may require a mask or stamp or some kind, e.g., injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, e.g., laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerisation, are called additive methods as they create the structure by building up the polymer structure.
{| class="wikitable"
|+
!
! [[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Additive/2PP|2 photon polymerisation]]
! [[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Additive/BMF|3D printers]]
|-
! scope=row style="text-align: left;" | Generel description
|
|
|-
! scope=row style="text-align: left;" | resolution
|
|
|-
! scope=row style="text-align: left;" | dimension
|
|
|-
! scope=row style="text-align: left;" | dimension
|
|
|-
! scope=row style="text-align: left;" | dimension
|
|
|-
! scope=row style="text-align: left;" | dimension
|
|
|-
! scope=row style="text-align: left;" | dimension
|
|
|}


==Coating==
In our Polyfablab, we have UV lithography, various additive methods, coating techniques, and imprinting techniques for polymer processing.
*[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Coating/Slot Die Coater|Slot Die Coater]]
*[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Coating/Parylene Coater|Parylene Coater]]
*[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Coating/Inkjet Printer|Inkjet Printer]]


==Imprinting==
==[[Specific_Process_Knowledge/Lithography/UVLithography|UV lithography]]==
*[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Imprinting/Imprinter 03|Imprinter 03 (200mm)]]
*[[Specific_Process_Knowledge/Lithography/UVExposure/aligner_MA6-1|Mask Aligner: MA6-1]]
*[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Imprinting/Imprinter 04|Imprinter 04 (110mm)]]
*[[Specific_Process_Knowledge/Lithography/UVExposure/aligner_MLA4|Maskless Aligner: μMLA-04]]
*[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Imprinting/Imprinter 05|Imprinter 05 (R2P)]]
*[[Specific_Process_Knowledge/Lithography/Coaters/labspin05|Labspin05]]


==Microscopes==
==[[Specific_Process_Knowledge/Polymer_Processing/Additive methods|Additive manufacturing methods]]==
*[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Microscopes/Microscope: Keyence VHX-X1|Microscope: Keyence VHX-X1]]
*[[Specific_Process_Knowledge/Polymer_Processing/Additive methods/Quantum X 2PP|Quantum X 2PP]]
*[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Microscopes/Laser Confocal Scanning Microscope|Laser Confocal Scanning Microscope]]
*[[Specific_Process_Knowledge/Polymer_Processing/Additive methods/3D Printer - BMF|3D Printer - BMF]]


==Plasma Cleaner==
==Coating methods==
*[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Plasma Cleaner/Plasma Cleaner 2: SurfacePrep|Plasma Cleaner 2: SurfacePrep]]
*[[Specific_Process_Knowledge/Polymer_Processing/Coating/Slot Die Coater|Slot Die Coater]]
*[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Plasma Cleaner 3/Plasma Cleaner 3: PDMS|Plasma Cleaner 3: PDMS]]
*[[Specific_Process_Knowledge/Polymer_Processing/Coating/Parylene Coater|Parylene Coater]]
*[[Specific_Process_Knowledge/Polymer_Processing/Coating/Inkjet Printer|Inkjet Printer]]


==[[Specific_Process_Knowledge/Imprinting|Imprinting]]==


<!--
==[[Specific_Process_Knowledge/Characterization/Optical microscope|Optical microscope]]==
[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Additive/2PP|2 photon polymerisation]]
[[Specific_Process_Knowledge/Polymer_Processing/PolyFabLab/Additive/BMF|3D printers]]
-->


= Polymer Processing =
==[[Specific_Process_Knowledge/Polymer_Processing/Plasma Cleaners|Plasma Cleaners]]==


There is a wide range of methods available to structure and modify polymers, though commonly done outside of a cleanroom.
==[[Specific_Process_Knowledge/Overview of Fume Hoods|Overview of Fume Hoods]]==


Many polymer processing methods may require a mask or stamp or some kind, f.ex. injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, f.ex. laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerization are called additive methods as they create the structure by a building up the polymer structure.
== Other Methods of Polymer Processing==
<br>
<br>
== Choose Method of Polymer Processing==
* [[Specific Process Knowledge/Lithography/NanoImprintLithography|Nano Imprint Lithography]]
* [[Specific Process Knowledge/Lithography/NanoImprintLithography|Nano Imprint Lithography]]
* [[Specific_Process_Knowledge/Back-end_processing/Hot_Embosser|Hot Embossing]] (Compression Molding)
* [[Specific_Process_Knowledge/Back-end_processing/Hot_Embosser|Hot Embossing]] (Compression Molding)
* [[Specific Process Knowledge/Characterization/Sample preparation| PDMS Casting I]]
* [[Specific_Process_Knowledge/Polymer_Processing/PDMS Casting|PDMS Casting II]]
* [[Specific Process Knowledge/Back-end processing/Polymer Injection Molder|Polymer Injection Molding]] ''(moved to DTU Construct))''
* [[Specific Process Knowledge/Back-end processing/Polymer Injection Molder|Polymer Injection Molding]] ''(moved to DTU Construct))''
* Polymer Casting (e.g. [[Specific Process Knowledge/Characterization/Sample preparation| PDMS Casting]])


'''Specialized Processes:'''
'''Specialized Processes:'''
* [[Specific Process Knowledge/Lithography/UVLithography|UV Lithography]]
* Additive Techniques
:* 3D printing
:* 2-Photon Polymerization Lithography
* Plasma Etching
* [[Specific Process Knowledge/Thin film deposition/MVD|FDTS coating (MVD)]]  
* [[Specific Process Knowledge/Thin film deposition/MVD|FDTS coating (MVD)]]  
* [[Specific Process Knowledge/Back-end processing/Laser Micromachining Tool|Laser Ablation/Milling]]
* [[Specific Process Knowledge/Back-end processing/Laser Micromachining Tool|Laser Ablation/Milling]]
Line 104: Line 54:
* Epoxy, e.g. SU-8
* Epoxy, e.g. SU-8
* Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc
* Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc
* Elastomer, e.g. PDMS
* Photo Resist, e.g. AZ resists
* Photo Resist, e.g. AZ resists

Latest revision as of 14:44, 28 September 2026

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

THIS PAGE IS UNDER CONSTRUCTION

Polymer Processing

Polymer processing involves transforming polymer resins into finished products with desired shapes, dimensions and performance characteristics. It combines the principles of polymer science, heat transfer, fluid mechanics, and manufacturing technology to produce a wide range of components for various applications. The processing conditions, such as temperature, pressure, and cooling rate, significantly influence the final properties of the polymer product.

There is a wide range of methods available to structure and modify polymers, though commonly done outside of a cleanroom, whereas some can be done inside a cleanroom.

Many polymer processing methods may require a mask or stamp or some kind, e.g., injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, e.g., laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerisation, are called additive methods as they create the structure by building up the polymer structure.

In our Polyfablab, we have UV lithography, various additive methods, coating techniques, and imprinting techniques for polymer processing.

UV lithography

Additive manufacturing methods

Coating methods

Imprinting

Optical microscope

Plasma Cleaners

Overview of Fume Hoods

Other Methods of Polymer Processing

Specialized Processes:


Choose Material for Polymer Processing

  • Epoxy, e.g. SU-8
  • Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc
  • Elastomer, e.g. PDMS
  • Photo Resist, e.g. AZ resists