Additive manufacturing enables the fabrication of three-dimensional structures directly from digital designs through layer-by-layer material deposition or polymerization. At PolyFabLab, additive manufacturing is primarily used for rapid prototyping, microfabrication, microfluidics, photonics, and advanced polymer device fabrication. | Additive manufacturing enables the fabrication of three-dimensional structures directly from digital designs through layer-by-layer material deposition or polymerization. At PolyFabLab, additive manufacturing is primarily used for rapid prototyping, microfabrication, microfluidics, photonics, and advanced polymer device fabrication. | ||
Latest revision as of 15:09, 25 September 2026
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
Additive manufacturing methods
Additive manufacturing enables the fabrication of three-dimensional structures directly from digital designs through layer-by-layer material deposition or polymerization. At PolyFabLab, additive manufacturing is primarily used for rapid prototyping, microfabrication, microfluidics, photonics, and advanced polymer device fabrication.
Currently, PolyFabLab offers two complementary additive manufacturing platforms:
Nanoscribe Quantum X align based on Two-Photon Polymerization (2PP) for ultra-high-resolution micro- and nanofabrication. Quantum X 2PP
Boston Micro Fabrication (BMF) microArch series based on Projection Micro Stereolithography (PµSL) for high-precision microscale 3D printing with larger build volumes and higher throughput. 3D Printer - BMF
The choice of equipment depends on the required feature size, build volume, material requirements, throughput, and alignment needs.
Comparion of Additive manufacturing methods
| Parameter | Quantum X 2PP | 3D Printer - BMF |
|---|---|---|
| Printing Principle | Laser-induced two-photon polymerization | UV projection stereolithography |
| Resoluation | Sub-micron to ~1 µm | 2 µm - 10 µm optical resolution |
| Alignment Capability | Excellent; automated alignment to fibers, chips, wafers and fiducials | Limited |
| Surface Quality | Extremely high | High |